Docol® 1200CP complex phase

Download data sheet

General Product Description

Docol 1200CP complex phase steel is developed for increased safety in cars. Its ultra-high strength combined with an improved formability allows for weight reduction in BIW applications. This steel undergoes special heat treatment in a continuous annealing or galvanizing line, producing a complex phase structure.

Dimension Range

Cold rolled / UC, EG: thickness 0.50-2.10 mm, width up to 1527 mm.

Cold rolled / GI: thickness 1.00-1.70 mm, width up to 1350 mm.

Slit strip are available upon request.

Grade and coating specific restrictions on available dimensions may occur.

Mechanical Properties

Docol CR​900Y​1180T-​CP

Standard
VDA 239-100
Coating
UC, EG, GI*
Test direction
L
Yield strength Rp0.2
(MPa)
900 - 1100
Tensile strength Rm
(MPa)
1180 - 1350
Elongation A80
(min %)
5
BH2
(min MPa)
30

The testing of mechanical properties of electrogalvanized products is conducted without coating.

* Available upon request

Chemical Composition (ladle analysis)

Docol CR​900Y​1180T-​CP

Coating
UC, EG, GI*
C
(max %)
0.23
Si
(max %)
1.00
Mn
(max %)
2.90
P
(max %)
0.050
S
(max %)
0.010
Al
(%)
0.015 - 1.00
Nb+Ti
(max %)
0.15
Cr+Mo
(max %)
1.00
B
(max %)
0.005
Cu
(max %)
0.20
* Available upon request.

Tolerances

Cold rolled (UC, EG): Tolerances in accordance to EN 10131.

Hot-dip galvanized (GI): Tolerances in accordance to EN 10143.

Customized dimensional and shape tolerances are available upon request.

Coatings

The metal coating options for Docol® products include:

Hot-dip zinc coating (GI) consists almost entirely of zinc (>99%). It is lead free, resulting in a small zinc spangle size. The coating provides good corrosion protection.

Electrogalvanized coating (EG) is applied continuously by electro deposition. The coating consists of zinc (>99%). Electrogalvanized steel is characterized by its excellent surface quality and uniform coating thickness.

Grade specific availability of metal coatings for Docol® products is given in the Mechanical properties table (Coating).

Coating type
Coating type
GI
Coating class
40/40
Standard
VDA 239-100
Closest in EN standard, informative 1)
Z100
Coating mass per side, single spot test (g/m2)
40 - 60
Thickness per side informative (µm)
5.6 - 8.5
Coating type
Coating type
GI
Coating class
50/50
Standard
VDA 239-100
Closest in EN standard, informative 1)
—
Coating mass per side, single spot test (g/m2)
50 - 70
Thickness per side informative (µm)
7.0 - 9.9
Coating type
Coating type
GI
Coating class
60/60
Standard
VDA 239-100
Closest in EN standard, informative 1)
Z140
Coating mass per side, single spot test (g/m2)
60 - 90
Thickness per side informative (µm)
8.5 - 12.7
Coating type
Coating type
GI
Coating class
70/70
Standard
VDA 239-100
Closest in EN standard, informative 1)
—
Coating mass per side, single spot test (g/m2)
70 - 100
Thickness per side informative (µm)
9.9 - 14.1
Coating type
Coating type
GI
Coating class
85/85
Standard
VDA 239-100
Closest in EN standard, informative 1)
—
Coating mass per side, single spot test (g/m2)
85 - 115
Thickness per side informative (µm)
12.0 - 16.2
Coating type
Coating type
GI
Coating class
115/115
Standard
VDA 239-100
Closest in EN standard, informative 1)
Z275
Coating mass per side, single spot test (g/m2)
115 - 155
Thickness per side informative (µm)
16.2 - 21.8
Coating type
Coating type
EG
Coating class
12/12
Standard
VDA 239-100
Closest in EN standard, informative 1)
ZE25/25
Coating mass per side, single spot test (g/m2)
12 - 32
Thickness per side informative (µm)
1.7 - 4.5
Coating type
Coating type
EG
Coating class
18/18
Standard
VDA 239-100
Closest in EN standard, informative 1)
—
Coating mass per side, single spot test (g/m2)
18 - 38
Thickness per side informative (µm)
2.5 - 5.4
Coating type
Coating type
EG
Coating class
29/29
Standard
VDA 239-100
Closest in EN standard, informative 1)
ZE50/50
Coating mass per side, single spot test (g/m2)
29 - 49
Thickness per side informative (µm)
4.1 - 6.9
Coating type
Coating type
EG
Coating class
47/47
Standard
VDA 239-100
Closest in EN standard, informative 1)
ZE75/75
Coating mass per side, single spot test (g/m2)
47 - 61
Thickness per side informative (µm)
6.6 - 8.6
Coating type
Coating type
EG
Coating class
50/50
Standard
VDA 239-100
Closest in EN standard, informative 1)
—
Coating mass per side, single spot test (g/m2)
50 - 70
Thickness per side informative (µm)
7.0 - 9.9
Coating type
Coating type
EG
Coating class
53/53
Standard
VDA 239-100
Closest in EN standard, informative 1)
—
Coating mass per side, single spot test (g/m2)
53 - 73
Thickness per side informative (µm)
7.5 - 10.3
Coating type
Coating type
EG
Coating class
60/60
Standard
VDA 239-100
Closest in EN standard, informative 1)
—
Coating mass per side, single spot test (g/m2)
60 - 80
Thickness per side informative (µm)
8.5 - 11.3
Coating type
Coating type
EG
Coating class
65/65
Standard
VDA 239-100
Closest in EN standard, informative 1)
ZE100/100
Coating mass per side, single spot test (g/m2)
65 - 85
Thickness per side informative (µm)
9.2 - 12.0
Coating type
Coating type
EG
Coating class
70/70
Standard
VDA 239-100
Closest in EN standard, informative 1)
—
Coating mass per side, single spot test (g/m2)
70 - 90
Thickness per side informative (µm)
9.9 - 12.7

Docol® metal coated products are available with surface quality for unexposed applications.

In addition to these coating masses, OEM specific coatings and single sided EG coatings are available upon request.

1) For GI and GA the closest informative value refers to EN 10346. For EG to EN 10152.

Surface Treatments

Uncoated (UC): available as oiled.

Hot-dip galvanized (GI): available as oiled and/or chemically passivated.

Electrogalvanized (EG): available as oiled and/or chemically passivated or phosphated.

All surface treatments are in accordance with RoHS directive (2011/65/EU) and do not contain Chromium VI (Cr6+). Surface treatments provide only temporary surface protection during transportation and storage. In order to avoid corrosion damages, care must be taken to keep the products dry during transportation and storage. If they become wet, they must be separated and situated so that they are dried quickly.

Fabrication and Other Recommendations

For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.

Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.

Docol® Complex Phase steel product offer

Docol® 600 CP complex phase

Visa produkten

Docol® 800CP complex phase

Visa produkten

Docol® 1000CP complex phase

Visa produkten

Docol® 1200CP complex phase

Visa produkten

Relaterat innehåll

AHSS provplåtslager

Vill du upptäcka unika biltillämpningar, prova nya produktionsmetoder eller skapa lättare komponenter som ger bättre bränsleeffektivitet, krockprestanda och hållbarhet?

Läs mer

Formningsdata för Docol® AHSS-stål

Befintliga Docol® kunder får tillgång till formningsdata dygnet runt för att underlätta deras val och simulering av avancerat höghållfast fordonsstål.

Läs mer