SSAB Boron Tube 24

Download data sheet

Select Language

Get datasheet by email
Close

Get datasheet by email

På denna sida

General Product Description

SSAB Boron Tube 24 is a structural hollow section for hardening. It offers good workshop properties in delivery condition. The degree of hardness and toughness that can be achieved after heat-treatment will provide the final products with wear- and shock resistance properties that assure longer lifetime.

Dimension Range

SSAB Boron Tube 24 is available at circular.

Hide/Show specific columns Edit
Select columns to display
    Shapes Dimensions
    Circular (mmin) 139.7 - 323.95.500 - 12.75
    Wall thickness (mmin) 5.0 - 10.00.20 - 0.394
    Mill length (mm) 6000/12000
    Compare parameters

    Select one parameter to compare

    Comparison

      Shapes
      Circular (mmin)
      Dimensions
      139.7 - 323.95.500 - 12.75
      Shapes
      Wall thickness (mmin)
      Dimensions
      5.0 - 10.00.20 - 0.394
      Shapes
      Mill length (mm)
      Dimensions
      6000/12000

      Other shapes, sizes and lengths are available upon request.

      Circular Dimensions

      Hide/Show specific columns Edit
      Select columns to display
        Outer diameter (mmin) 5.0 mm (kg/m) 6.0 mm (kg/m) 8.0 mm (kg/m) 10.0 mm (kg/m)
        139.75.500 19.8
        168.36.626 24.0
        219.18.626 26.4 31.5 41.7 51.6
        27310.7 39.5 52.3
        323.912.75 47.0 62.3
        Compare parameters

        Select one parameter to compare

        Comparison

          Mechanical Properties

          Hide/Show specific columns Edit
          Select columns to display
            Condition Typical yield strength
            (MPa), not guaranteed
            Typical tensile strength
            (MPa), not guaranteed
            Typical Elongation A (%),
            not guaranteed
            As delivered 470 650 12
            Compare parameters

            Select one parameter to compare

            Comparison

              Typical mechanical properties when quenched to water:

              Rp0.2 ~1100 MPa; Rm ~1400 MPa; A~8%

              Chemical Composition (ladle analysis)

              Hide/Show specific columns Edit
              Select columns to display
                C
                (max %)
                Si
                (max %)
                Mn
                (max %)
                S
                (max %)
                Cr
                (max %)
                B
                (max %)
                P
                (max %)
                0.27 0.30 1.20 0.010 0.40 0.0050 0.020
                Compare parameters

                Select one parameter to compare

                Comparison

                  Tolerances

                  Tolerance Circular

                  Hide/Show specific columns Edit
                  Select columns to display
                    Characteristic Circular hollow sections
                    Tolerances meet or exceed the requirements of EN 10219
                    Outside diameter (D) (1 ±1%, with a minimum of ±0.5 mm and a maximum of ±10 mm
                    Out-of-roundness 2%, when D/T ≤ 100
                    Thickness (T) When D ≤ 323.9 mm: -5%/+10%, with a minimum of ±0.2 mm and maximum ±0.5 mm
                    When 355.6 ≤ D ≤ 406.4 mm : ±10%, when T ≤ 5 mm / ±0.5 mm, when T > 5 mm
                    When D > 406.4 mm : ±10%, with a maximum of ±2 mm
                    Straightness 0.20% of total length and 3 mm over any 1 m length
                    Mass per unit length Individual tube: ±6%
                    Mill length 0/+50 mm, 6000 ≤ L ≤ 12000 - 18000 mm (standard lengths 6000 & 12000 mm)
                    Exact length Agreed at the time of enquiry and order
                    Compare parameters

                    Select one parameter to compare

                    Comparison

                      Characteristic
                      Outside diameter (D) (1
                      Circular hollow sections
                      Tolerances meet or exceed the requirements of EN 10219
                      ±1%, with a minimum of ±0.5 mm and a maximum of ±10 mm
                      Characteristic
                      Out-of-roundness
                      Circular hollow sections
                      Tolerances meet or exceed the requirements of EN 10219
                      2%, when D/T ≤ 100
                      Characteristic
                      Thickness (T)
                      Circular hollow sections
                      Tolerances meet or exceed the requirements of EN 10219
                      When D ≤ 323.9 mm: -5%/+10%, with a minimum of ±0.2 mm and maximum ±0.5 mm
                      When 355.6 ≤ D ≤ 406.4 mm : ±10%, when T ≤ 5 mm / ±0.5 mm, when T > 5 mm
                      When D > 406.4 mm : ±10%, with a maximum of ±2 mm
                      Characteristic
                      Straightness
                      Circular hollow sections
                      Tolerances meet or exceed the requirements of EN 10219
                      0.20% of total length and 3 mm over any 1 m length
                      Characteristic
                      Mass per unit length
                      Circular hollow sections
                      Tolerances meet or exceed the requirements of EN 10219
                      Individual tube: ±6%
                      Characteristic
                      Mill length
                      Circular hollow sections
                      Tolerances meet or exceed the requirements of EN 10219
                      0/+50 mm, 6000 ≤ L ≤ 12000 - 18000 mm (standard lengths 6000 & 12000 mm)
                      Characteristic
                      Exact length
                      Circular hollow sections
                      Tolerances meet or exceed the requirements of EN 10219
                      Agreed at the time of enquiry and order

                      1) All external dimensions are measured with a minimum distance from the end of the section. The distance must be a minimum of 100 mm.

                      Contact Information