Docol® 500LA high strength low alloy

Download data sheet

General Product Description

The Docol 500LA steels are high-strength low-alloy steels that offer consistent properties for modern, rapid production methods. Typical applications include bent profiles. Docol HR500LA-UC can after agreement be adapted and delivered as dual certified with S500MC according to EN 10149-2.

Dimension Range

Hot rolled / UC: thickness 2.00-6.00 mm, width up to 1600 mm.

Slit strip and cut to length sheets are available upon request.

Grade and coating specific restrictions on available dimensions may occur.

Mechanical Properties

Docol HR​500LA

Standard
VDA 239-100
Coating
UC
Test direction
L
Yield strength Rp0.2
(MPa)
500 - 620
Tensile strength Rm
(MPa)
560 - 700
Elongation A80 1)
(min %)
14
Elongation A5 2)
(min %)
17
Min. inner bending radius for a 90° bend
0.8 x t

1) A80 value applies for thicknesses < 3.00 mm.

2) A5 value applies for thicknesses ≥ 3.00 mm.

Chemical Composition (ladle analysis)

Docol HR​500LA

Coating
UC
C
(max %)
0.10
Si
(max %)
0.50
Mn
(max %)
1.60
P
(max %)
0.025
S
(max %)
0.010
Al
(%)
From 0.015
Ti
(max %)
0.15
Nb
(max %)
0.10
Cu
(max %)
0.20

Tolerances

Hot rolled (UC): Tolerances in accordance to EN 10051.

Customized dimensional and shape tolerances are available upon request.

Surface Treatments

Uncoated (UC): available as oiled.

All surface treatments are in accordance with RoHS directive (2011/65/EU) and do not contain Chromium VI (Cr6+). Surface treatments provide only temporary surface protection during transportation and storage. In order to avoid corrosion damages, care must be taken to keep the products dry during transportation and storage. If they become wet, they must be separated and situated so that they are dried quickly.

Fabrication and Other Recommendations

For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.

Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.

Docol® High Strength Low Alloy steel product offer

Docol® 420LA high strength low alloy

Visa produkten

Docol HR100XF

Visa produkten

Docol HR110XF

Visa produkten

Docol® S600MC high strength low alloy

Visa produkten

Docol® S650MC high strength low alloy

Visa produkten

Docol® S700MC high strength low alloy

Visa produkten

Docol® S900MC high strength low alloy

Visa produkten

Docol S960MC

Visa produkten

Docol® 460LA high strength low alloy

Visa produkten

Docol® 500LA high strength low alloy

Visa produkten

Docol® 550LA high strength low alloy

Visa produkten

Docol® 600LA high strength low alloy

Visa produkten

Docol® 650LA high strength low alloy

Visa produkten

Docol® 700LA high strength low alloy

Visa produkten

Relaterat innehåll

AHSS provplåtslager

Vill du upptäcka unika biltillämpningar, prova nya produktionsmetoder eller skapa lättare komponenter som ger bättre bränsleeffektivitet, krockprestanda och hållbarhet?

Läs mer

Formningsdata för Docol® AHSS-stål

Befintliga Docol® kunder får tillgång till formningsdata dygnet runt för att underlätta deras val och simulering av avancerat höghållfast fordonsstål.

Läs mer