SSAB Domex Tube 355 J2H

SSAB Domex® Tube 355J2H

Hollow section for general applications

SSAB Domex® Tube 355J2H is cold formed advanced structural hollow section

It meets or exceeds the requirements of standard EN 10219 and is available in circular, rectangular, square and special shapes. It is typically used in advanced engineering and construction where lower costs and safety are important. It has very clean chemistry and uniform quality. The impact ductility is tested at -40°C and it is suitable for hot-dip galvanizing. Also welding in corner areas is always permitted.

SSAB Domex® Tube 355J2H is manufactured by cold forming and high frequency welding from clean, high quality environmentally friendly steel by modern and efficient tube lines.

Dimension Range

SSAB Domex Tube 355J2H is available at circular, square and rectangular shapes. 

   
Circular 42.4 - 323.9 mm 
Square 40x40 - 300x300 mm 
Rectangular 50x30 - 400x200 mm 
Wall thickness 2.0 - 12.50 mm
Mill length 6000/12 000 mm

Other shapes, sizes and lengths are available upon request.

Tillgängliga standarder

EN 10219-1

EN 10219-2

Välj form för att visa egenskaper