SSAB Domex® Tube 460MH

Download data sheet

Select Language

Get datasheet by email
Close

Get datasheet by email

På denna sida

General Product Description

SSAB Domex Tube 460MH is high strength structural hollow section.

It meets or exceeds the requirements of EN 10219 and is available in circular, rectangular, square and special shapes. Customized shapes and other tailoring options are available upon request. It is typically used in advanced engineering and construction where weight reduction, lower costs and safety are important.

SSAB Domex Tube 460MH is manufactured by cold forming and high frequency welding from clean, high quality environmentally friendly steel by modern and efficient tube lines.

Dimension Range

SSAB Domex Tube 460MH is available in circular, square and rectangular shapes.

Hide/Show specific columns Edit
Select columns to display
    Shapes Dimensions
    Circular (mmin) 42.4 - 323.91.67 - 12.75
    Square (mmin) 40x40 - 300x300
    Rectangular (mmin) 50x30 - 400x200
    Wall thickness (mmin) 2.0 - 12.50.079 - 0.492
    Mill length (mm) 6000 - 12 000/18 000 mm
    Compare parameters

    Select one parameter to compare

    Comparison

      Shapes
      Circular (mmin)
      Dimensions
      42.4 - 323.91.67 - 12.75
      Shapes
      Square (mmin)
      Dimensions
      40x40 - 300x300
      Shapes
      Rectangular (mmin)
      Dimensions
      50x30 - 400x200
      Shapes
      Wall thickness (mmin)
      Dimensions
      2.0 - 12.50.079 - 0.492
      Shapes
      Mill length (mm)
      Dimensions
      6000 - 12 000/18 000 mm

      Other shapes, sizes and lengths are available upon request.

      Circular Dimensions

      Hide/Show specific columns Edit
      Select columns to display
        Outer diameter (mmin) 2.0 mm (kg/m) 3.0 mm (kg/m) 4.0 mm (kg/m) 5.0 mm (kg/m) 6.0 mm (kg/m) 8.0 mm (kg/m) 10.0 mm (kg/m) 12.5 mm (kg/m)
        42.41.67 1.99 2.19
        48.31.90 2.28 3.35 4.37
        60.32.37 2.88 4.24 5.55 6.82
        76.13.00 5.41 7.11
        88.93.50 6.36 8.38 10.4
        101.64.000 7.29 9.63 11.9
        1084.25 7.77 10.3 12.7
        114.34.500 8.23 10.9 13.5
        1275.00 9.17 12.1 15.0
        139.75.500 13.4 16.6 19.8 26.0 32.0
        168.36.626 16.2 20.1 24.0 31.6 39.0
        219.18.626 26.4 31.5 41.7 51.6
        27310.7 33.1 39.5 52.3 64.9 80.3
        323.912.75 47.0 62.3 77.4 96.0
        Compare parameters

        Select one parameter to compare

        Comparison

          Square Dimensions

          Hide/Show specific columns Edit
          Select columns to display
            Height x Width (mm) 2.0 mm (kg/m) 3.0 mm (kg/m) 4.0 mm (kg/m) 5.0 mm (kg/m) 6.0 mm (kg/m) 8.0 mm (kg/m) 10.0 mm (kg/m) 12.5 mm (kg/m)
            40 x 40 2.31 3.30 4.20
            50 x 50 2.93 4.25 5.45
            60 x 60 3.56 5.19 6.71 8.13
            70 x 70 6.13 7.97 9.70
            80 x 80 7.07 9.22 11.3 13.2
            90 x 90 8.01 10.5 12.8 15.1
            100 x 100 8.96 11.7 14.4 17.0 21.4
            120 x 120 14.3 17.6 20.8 26.4
            140 x 140 16.8 20.7 24.5 31.4 38.1
            150 x 150 18.0 22.3 24.5 31.4 41.3
            160 x 160 23.8 28.3 36.5 44.4 52.6
            180 x 180 27.0 32.1 41.5 50.7 60.5
            200 x 200 30.1 35.8 46.5 57.0 68.3
            250 x 250 45.2 59.1 72.7 88.0
            300 x 300 54.7 71.6 88.4 108
            Compare parameters

            Select one parameter to compare

            Comparison

              Rectangular Dimensions

              Hide/Show specific columns Edit
              Select columns to display
                Height x Width (mm) 2.0 mm (kg/m) 3.0 mm (kg/m) 4.0 mm (kg/m) 5.0 mm (kg/m) 6.0 mm (kg/m) 8.0 mm (kg/m) 10.0 mm (kg/m) 12.5 mm (kg/m)
                50 x 30 2.31 3.30 4.20
                60 x 40 2.93 4.25 5.45 6.56
                80 x 40 3.56 5.19 6.71 8.13
                80 x 60 6.13 7.97 9.70
                100 x 50 6.60 8.59 10.5
                100 x 60 7.07 9.22 11.3
                100 x 80 8.01 10.5 12.8
                120 x 60 8.01 10.5 12.8
                120 x 80 8.96 11.7 14.4
                140 x 80 13.0 16.0
                150 x 100 14.9 18.3 21.7 27.7
                160 x 80 14.3 17.6 20.8 26.4
                180 x 100 20.7 24.5 31.4 38.1
                200 x 100 22.3 26.4 34.0 41.3
                200 x 120 23.8 28.3 36.5 44.4 52.6
                250 x 100 26.18 31.11 40.23 49.11
                250 x 150 30.1 35.8 46.5 57.0 68.3
                300 x 200 45.2 59.1 72.7 88.0
                400 x 200 54.7 71.6 88.4 108
                Compare parameters

                Select one parameter to compare

                Comparison

                  Mechanical Properties

                  Hide/Show specific columns Edit
                  Select columns to display
                    Yield strength Rp0.2
                    (min MPa)
                    Tensile strength Rm
                    (MPa)
                    Elongation A5 1)
                    (min %)
                    Charpy-V -40°C 10x10 mm test specimen 2)
                    (J)
                    460 530 - 720 17 27
                    </