SSAB Boron Tube 22
Offers good formability in delivery condition and ultra-high strength as quenched
SSAB Boron Tube 22 is hardenable precision tube. It offers good formability in delivery condition and ultra-high strength by quenching after work shop fabrications.
Available in circular, rectangular, square and special shapes. Customized shapes and other tailoring options are available upon request. It is typically used in safety structures in vehicles and light engineering when uttermost strength and wear resistant are needed.
SSAB Boron Tube 22 is manufactured from clean, high quality environmentally friendly steel by modern and efficient tube lines.