Product Name | Dimensions | Standards | Datasheet |
|---|---|---|---|
| SSAB Weathering Tube 320WP | Circular: 16 - 88.9 mm Square: 19x19 - 70x70 mm Rectangular: 25x15 - 100x40 mm Wall Thickness: 1.0 - 3.0 mmCircular: 0.63 - 3.50 in Square: in Rectangular: in Wall Thickness: 0.039 - 0.12 in | EN 10305-3 | |
| SSAB Weathering Tube 355WH | Circular: 48.3 - 323.9 mm Square: 40x40 - 300x300 mm Rectangular: 50x30 - 400x200 mm Wall Thickness: 2.0 - 12.5 mmCircular: 1.90 - 12.75 in Square: in Rectangular: in Wall Thickness: 0.079 - 0.492 in | EN 10219 | |
| SSAB Weathering Tube 500WH | Circular: 48.3 - 323.9 mm Square: 40x40 - 300x300 mm Rectangular: 50x30 - 400x200 mm Wall Thickness: 2.0 - 12.5 mmCircular: 1.90 - 12.75 in Square: in Rectangular: in Wall Thickness: 0.079 - 0.492 in | EN 10219 | |
| SSAB COR-TEN B Tube | Circular: 48.3 - 323.9 mm Square: 40x40 - 300x300 mm Rectangular: 50x30 - 400x200 mm Wall Thickness: 2.0 - 12.5 mmCircular: 1.90 - 12.75 in Square: in Rectangular: in Wall Thickness: 0.079 - 0.492 in | EN 10219 |
SSAB Weathering Tube 320WP
SSAB Weathering Tube 355WH
SSAB Weathering Tube 500WH
SSAB COR-TEN B Tube