Tubes product group

Product Name

SSAB Form Tube 220

Dimensions
Circular: 16 - 88.9 mm
Square: 19x19 - 70x70 mm
Rectangular: 25x15 - 100x40 mm
Flat oval: 25x15 - 78x38 mm
Oval: 22x16.5 - 31x17.5 mm
Wall Thickness: 0.9 - 3.0 mm
Circular: 0.63 - 3.50 in
Square: in
Rectangular: in
Flat oval: in
Oval: in
Wall Thickness: 0.04 - 0.12 in
Standards
EN 10305-3
Datasheet
Product Name

SSAB Form Tube 320

Dimensions
Circular: 16 - 88.9 mm
Square: 19x19 - 70x70 mm
Rectangular: 25x15 - 100x40 mm
Flat oval: 25x15 - 78x38 mm
Oval: 22x16.5 - 31x17.5 mm
Wall Thickness: 0.9 - 3.0 mm
Circular: 0.63 - 3.50 in
Square: in
Rectangular: in
Flat oval: in
Oval: in
Wall Thickness: 0.04 - 0.12 in
Standards
EN 10305-3
Datasheet
Product Name

SSAB Form Tube 420

Dimensions
Circular: 16 - 88.9 mm
Square: 19x19 - 70x70 mm
Rectangular: 25x15 - 100x40 mm
Wall Thickness: 0.9 - 3.0 mm
Circular: 0.63 - 3.50 in
Square: in
Rectangular: in
Wall Thickness: 0.04 - 0.12 in
Standards
EN 10305-3
Datasheet