SSAB Epoxy color coated steel from SSAB is available in regular and matt finishes. It is used in different indoor building applications, but also in other industries like inside walls for passenger buses. 

SSAB Epoxy color coated steel is well suited for objects that are later finished with the color chosen by the customer. It can also be used in indoor applications where wallboards or tiles are bonded on the surface. Light washing is enough as a pre-treatment. 

SSAB Epoxy color coated steel offers good adhesion and corrosion resistance.

The reverse side of the sheet is painted with a two-layer grey backside coating.

SSAB Epoxy complies with current REACH regulations and is fully free of chromates.

SSAB’s color coated steels are all manufactured according to EN 10169.

Technical Properties

Technical Properties
Technical Properties
Gloss
Regular
35
Matt
10
Technical Properties
Technical Properties
Minimum inner bending radius
Regular
5 x sheet thickness
Matt
5 x sheet thickness
Technical Properties
Technical Properties
Corrosion resistance
Regular
Min CPI3
Matt
Min CPI3
Technical Properties
Technical Properties
Highest operating temperature
Regular
110 °C
Matt
110 °C
Technical Properties
Technical Properties
Coating thickness, nominal (primer + top coat)
Regular
12 µm
Matt
12 µm

Colors

SSAB Epoxy is available in standard grey (reverse side color). Other colors can be agreed upon separately.

Reverse Side Coating

Technical Properties
Technical Properties
Nominal Coating Thickness (primer + top coat)
12 µm
Technical Properties
Technical Properties
Color
Grey
Technical Properties
Technical Properties
Corrosion Resistance
Min CPI3