How to weld > Welding consumables

The toughness values in the weld metal

The consumables with the appropriate strengths for welding the Hardox® wear plate and Strenx® performance steel grades can, in many cases, attain favorable toughness values in the all weld metal.
The weld metal in joints of the Strenx® performance steel grades can reach an impact toughness – with many kinds of consumables – that is typically above the toughness requirements of the unaffected parent metal.

There are seldom exact, specified toughness requirements for joints in the Hardox® wear plate grades. When measured, the impact toughness values in the weld metal are normally at a level of – or above – the typical impact toughness values for these steel grades.

Contact Technical support


The information in this report is only applicable to SSAB’s products and should not be applied to any other products than original SSAB products. 


This report provides general results and recommendations for SSAB steel products. This report is subject to SSAB’s Terms of Use. It shall be the user's responsibility to verify that the information contained herein is correct and is suitable to be used for the particular purpose and application of the user. The report is intended to be used by professional users only who possess adequate expertise, qualification and knowledge for the safe and correct use of the results and recommendations in this report. This report is provided “as is”. The use of the report is at user’s own discretion and risk and that users will be solely responsible for any use of this report. SSAB disclaims any liability for the content or potential errors of this report, including but not limited to warranties and condition of merchantability or fitness for a particular purpose or suitability for individual applications. SSAB shall not be liable for any kind of direct or indirect damages and/or costs related to or arising therefrom, whether special, incidental, consequential or directly or indirectly related to the use of, or the inability to use, the report or the content, information or results included therein. 