The SSAB Weathering portfolio includes a wide range of heavy plate, hot and cold rolled strip, tube and sections with yield strength from 355 to 550 MPa.
Weather-resistant steel from SSAB is easy to work with and give your products and installations the long-term performance you are looking for.
SSAB Weathering has excellent properties for forming, machining and welding. The SSAB Weathering portfolio includes a wide range of grades with mechanical properties and dimensional tolerances that generally exceed the standards given by EN 10025-5, and ASTM grades.
SSAB Weathering steel grades are available from stock or mill. You can also order a trial delivery for testing in your production.
Your local service contact will answer any questions about ordering and shipping, delivery times, marking and packing.
Contact usSSAB Weathering 355
SSAB Weathering 420
SSAB Weathering 460
SSAB Weathering 550
SSAB Weathering 355NL
SSAB Weathering 355ML
SSAB Weathering 420ML
SSAB Weathering 460ML
SSAB Weathering Tube 320WP