SSAB Form Tube 320

Download data sheet

Select Language

Get datasheet by email
Close

Get datasheet by email

On this page

General Product Description

Form Tube 320 is a formable precision tube. It has 20% higher elongation values and very narrow tolerances compared to competing products. Available in circular, rectangular, square and special shapes, it comes with different coating and surface options including cold rolled, galvanized, galvannealed and galfan. Customized shapes and other tailoring options are available upon request. Typically uses include light engineering, where formability, uniform quality, different surface options and usability are important.

Dimension Range

SSAB Form Tube 320 is available in circular, square, rectangular, flat oval and oval (elliptic) shapes.

Hide/Show specific columns Edit
Select columns to display
    Shapes Dimensions
    Circular (mmin) 16 - 88.90.63 - 3.50
    Square (mmin) 19x19 - 70x70
    Rectangular (mmin) 25x15 - 100x40
    Flat oval (mm) 25x15 - 78x38
    Oval, elliptic (mm) 22x16.5 - 31x17.5
    Wall thickness (mmin) 0.9 - 3.00.04 - 0.12
    Mill length (mm) 6000
    Compare parameters

    Select one parameter to compare

    Comparison

      Shapes
      Circular (mmin)
      Dimensions
      16 - 88.90.63 - 3.50
      Shapes
      Square (mmin)
      Dimensions
      19x19 - 70x70
      Shapes
      Rectangular (mmin)
      Dimensions
      25x15 - 100x40
      Shapes
      Flat oval (mm)
      Dimensions
      25x15 - 78x38
      Shapes
      Oval, elliptic (mm)
      Dimensions
      22x16.5 - 31x17.5
      Shapes
      Wall thickness (mmin)
      Dimensions
      0.9 - 3.00.04 - 0.12
      Shapes
      Mill length (mm)
      Dimensions
      6000

      Other shapes, sizes and lengths are available upon request.

      Circular Dimensions

      Hide/Show specific columns Edit
      Select columns to display
        Outer diameter (mmin) 0.9 mm (kg/m) 1.0 mm (kg/m) 1.25 mm (kg/m) 1.5 mm (kg/m) 2.0 mm (kg/m) 2.5 mm (kg/m) 3.0 mm (kg/m)
        160.63 0.335 0.370 0.455 0.536 0.691 1)
        180.71 0.380 0.419 0.516 0.610 0.789
        190.75 0.402 0.444 0.547 0.647 0.838
        200.79 0.424 0.469 0.578 0.684 0.888
        220.87 0.468 0.518 0.640 0.758 0.986 1.20 1.41 1)
        250.98 0.535 0.592 0.732 0.869 1.13 1.39 1.63 1)
        281.1 0.601 0.666 0.825 0.980 1.28 1.57 1.85
        301.2 0.646 0.715 0.886 1.05 1.38 1.70 2.00
        321.3 0.765 0.948 1.13 1.48 1.82 2.15
        351.4 0.838 1.04 1.24 1.63 2.00 2.37
        381.5 0.912 1.13 1.35 1.78 2.19 2.59
        401.6 0.962 1.20 1.42 1.87 2.31 2.74
        411.6 0.990 1.22 1.46 1.92 2.37 2.81
        41.51.63 0.999 1.24 1.48 1.95 2.40 2.85
        44.51.75 1.07 1.33 1.59 2.10 2.59 3.07
        481.9 1.44 1.72 2.27 2.81 3.33
        502.0 1.50 1.79 2.37 2.93 3.48
        50.82.00 1.53 1.82 2.41 2.98 3.54
        552.2 1.66 1.98 2.61 3.24 3.85
        572.2 1.72 2.05 2.71 3.36 4.00
        602.4 1.81 2.16 2.86 3.55 4.22
        702.8 2.53 3.35 4.16 4.96
        76.13.00 2.76 3.65 4.54 5.41
        88.93.50 4.29 5.33 6.36
        Compare parameters

        Select one parameter to compare

        Comparison