Ramor® SR500

Download data sheet

General Product Description

Ramor® SR500 is a ballistic steel well suited for shooting ranges, shooting targets etc.

 

Dimension Range

Ramor® SR500 is available as plate in thicknesses of 4.8 - 12.7 mm (0.188 - 0.500").
Dimensions upon agreement.

 

Mechanical Properties

Product
Product
Ramor® SR500
Hardness
(HBN)
500 - 590
Typical impact toughness, Charpy-V 10x10mm
30 J / -20 °C8 ft-lbs / -4 °F
Typical yield strength Rp0.2 (MPaksi)
1400203
Typical tensile strength Rm (MPaksi)
1800261
Typical elongation A5
(%)
10

 

Chemical Composition

C
(max %)
C
(max %)
0.32
Mn
(max %)
1.6
Si
(max %)
0.7
Cr
(max %)
2.0
CE(IIW) Typical
0.7

 

 

Tolerances

Thickness, width and length tolerances are in accordance with ASTM A6.

Flatness tolerances according to ASTM A6.

 

Delivery Conditions

Plates are delivered in quenched or quenched and tempered condition.

 