Product offer and datasheets

SSAB Domex Tubes

Product Name

SSAB Domex Tube 355J2H

Dimensions
Circular: 42.4 - 323.9 mm
Square: 40x40 - 300x300 mm
Rectangular: 50x30 - 400x200 mm
Wall Thickness: 2.0 - 12.5 mm
Circular: 1.67 - 12.75 in
Square: in
Rectangular: in
Wall Thickness: 0.079 - 0.492 in
Standards
EN 10219-1, EN 10219-2
Datasheet
Product Name

SSAB Domex Tube Double Grade

Dimensions
Circular: 42.4 - 323.9 mm
Square: 40x40 - 300x300 mm
Rectangular: 50x30 - 400x200 mm
Wall Thickness: 2.0 - 12.50 mm
Circular: 1.67 - 12.75 in
Square: in
Rectangular: in
Wall Thickness: 0.079 - 0.4921 in
Standards
EN 10219-1, EN 10219-2
Datasheet
Product Name

SSAB Domex Tube 460MH

Dimensions
Circular: 42.4 - 323.9 mm
Square: 40x40 - 300x300 mm
Rectangular: 50x30 - 400x200 mm
Wall Thickness: 2.0 - 12.5 mm
Circular: 1.67 - 12.75 in
Square: in
Rectangular: in
Wall Thickness: 0.079 - 0.492 in
Standards
EN 10219-1, EN 10219-2
Datasheet
Product Name

SSAB Domex Tube 500MH

Dimensions
Circular: 42.4 - 323.9 mm
Square: 40x40 - 300x300 mm
Rectangular: 50x30 - 400x200 mm
Wall Thickness: 2.0 - 12.5 mm
Circular: 1.67 - 12.75 in
Square: in
Rectangular: in
Wall Thickness: 0.079 - 0.492 in
Standards
EN 10219-2, EN 1090-2
Datasheet
Product Name

SSAB Domex Tube 550MH

Dimensions
Circular: 42.4 - 323.9 mm
Square: 40x40 - 300x300 mm
Rectangular: 50x30 - 400x200 mm
Wall Thickness: 2.0 - 12.50 mm
Circular: 1.67 - 12.75 in
Square: in
Rectangular: in
Wall Thickness: 0.079 - 0.4921 in
Standards
EN 10219-2, EN 1090-2
Datasheet

SSAB Weathering Tubes

Product Name

SSAB Weathering Tube 355WH

Dimensions
Circular: 48.3 - 323.9 mm
Square: 40x40 - 300x300 mm
Rectangular: 50x30 - 400x200 mm
Wall Thickness: 2.0 - 12.5 mm
Circular: 1.90 - 12.75 in
Square: in
Rectangular: in
Wall Thickness: 0.079 - 0.492 in
Standards
EN 10219
Datasheet
Product Name

SSAB Weathering Tube 500WH

Dimensions
Circular: 48.3 - 323.9 mm
Square: 40x40 - 300x300 mm
Rectangular: 50x30 - 400x200 mm
Wall Thickness: 2.0 - 12.5 mm
Circular: 1.90 - 12.75 in
Square: in
Rectangular: in
Wall Thickness: 0.079 - 0.492 in
Standards
EN 10219
Datasheet
Product Name

SSAB COR-TEN B Tube

Dimensions
Circular: 48.3 - 323.9 mm
Square: 40x40 - 300x300 mm
Rectangular: 50x30 - 400x200 mm
Wall Thickness: 2.0 - 12.5 mm
Circular: 1.90 - 12.75 in
Square: in
Rectangular: in
Wall Thickness: 0.079 - 0.492 in
Standards
EN 10219
Datasheet

Strenx Tubes

Product Name

Strenx® Tube 700MLH

Thickness range (mmin)
2.5 - 10.00.098 - 0.393
Circular (mmin)
48.3 - 323.91.669 - 12.752
Square (mmin)
40x40 - 300x3001.575x1.575 - 11.811x11.811
Rectangular (mmin)
50x30 - 400x2001.969x1.181 - 15.748x7.874
Yield strength (min MPaksi)
700101
Standards
EN 10219-3
Shapes
Circular, Rectangular, Square
Datasheet
Product Name

Strenx® Tube 900MH

Thickness range (mmin)
4.0 - 6.00.157 - 0.236
Circular (mmin)
139.7 - 219.15.500 - 8.626
Square (mmin)
100x100 - 200x2003.937x3.937 - 7.874x7.874
Rectangular (mmin)
120x80 - 250x1504.724x3.149 - 9.843x5.906
Yield strength (min MPaksi)
900130
Standards
EN 10219-3
Shapes
Circular, Rectangular, Square
Datasheet
Product Name

Strenx® Tube 960MH

Thickness range (mmin)
4.0 - 6.00.157 - 0.236
Circular (mmin)
139.7 - 219.15.500 - 8.626
Square (mmin)
100x100 - 200x2003.937x3.937 - 7.874x7.874
Rectangular (mmin)
120x80 - 250x1504.724x3.149 - 9.843x5.906
Yield strength (min MPaksi)
960139
Standards
EN 10219-3
Shapes
Circular, Rectangular, Square
Datasheet
Product Name

Strenx® Tube 960QLH

Thickness range (mmin)
3.0 - 6.00.118 - 0.236
Circular (mmin)
76.1 - 133.03.000 - 5.236
Square (mmin)
-
Rectangular (mmin)
-
Yield strength (min MPaksi)
960140
Standards
EN 10210
Shapes
Circular
Datasheet