Steel Processing

SSAB Steel Service Center in Oborniki, Poland has a wide range of steel processing capabilities. From shot blasting and cutting to bending, drilling, machining and much more.

Shot Blasting

Steel processing - shot blasting

If requested, we can shot blast each plate entering our facility, to ensure premium Surface condition of each part. We use Schlick shot blasting line with following parameters:

PLATE THICKNESS RANGE: 6–200 mm
PLATE WIDTH: 2500 mm
PLATE MAXIMUM WEIGHT: 10 000 kg
ABRASIVE MEDIUM: Steel, Sa 2.5

Cutting

Steel processing - Flame cutting

Flame (oxygen) cutting

Depending on the part specification, plate thickness and customers’ requirements, we can use the following thermal cutting methods in our facility.

MANUFACTURER: Messer
TABLE SIZE: 2500x13000 mm
NO OF TORCHES: 4
BEVELIING: flame or mechanical
TOLERANCES: EN 9013-1 Class 2

MANUFACTURER: Messer
TABLE SIZE: 5000x13000 mm
NO OF TORCHES: 12
BEVELIING: flame or mechanical
TOLERANCES: EN 9013-1 Class 2

Steel processing - Plasma cutting

Plasma cutting

Depending on the part specification, plate thickness and customers’ requirements we can use the following thermal cutting methods in our facility.

MANUFACTURER: ESAB
TABLE SIZE: 3000x14000mm
PLASMA TORCH: 3D torch  540 , cuting angle up to 45 
PLASMA SOURCE: ESAB 450A
OXY-GEN TORCHES: 2
TOLERANCES: EN 9013-1 Class 2

MANUFACTURER: Messer
TABLE SIZE: 2500x13000mm
NO OF TORCHES: 2
PLASMA SOURCE: Hypertherm 260A
TOLERANCES: EN 9013-1 Class 2

MANUFACTURER: Messer
TABLE SIZE: 5000x13000mm
NO OF TORCHES: 2
PLASMA SOURCE: Hypertherm 260A
TOLERANCES: EN 9013-1 Class 2

Steel processing - Laser cutting

Laser cutting

Depending on the part specification, plate thickness and customers’ requirements, we can use the following thermal cutting methods in our facility.

MANUFACTURER: Messer
TABLE SIZE: 4100x14000 mm
LASER: Fanuc CO2 6 kw, 3D endless rotating bevel head
TOLERANCES: EN 9013-1 Class 1

Bending

Steel processing - Bending

Bending

Depending on the part specification, plate thickness and customers’ requirements, we can use one of the following press brakes:

MANUFACTURER: Ursviken
BENDING LENGTH: 12200 mm
DISTANCE BETWEEN COLUMNS: 10200 mm
MAXIMUM PRESS POWER: 2000 ton
VARIABLE DIE SCOPE: 40-300 mm
Flexicrown – precise deflection control
Ecopump – Energy saving ecological pump
6-axis CNC controlled back gauge

MANUFACTURER: Durma
BENDING LENGTH: 10500 mm
DISTANCE BETWEEN COLUMNS: 9000 mm
MAXIMUM PRESS POWER: 1500 ton

MANUFACTURER: Aliko
BENDING LENGTH: 4000 mm
MAXIMUM PRESS POWER: 400 ton 

Drilling, Machining & Other

Steel processing - Drilling

Depending on specific needs and requirements, we can provide further precise processing, such as:

Drilling with Pax radial drilling machine, which we use for drilling, threading, counterboring and other operations in mild
steels, high-strength steels and Hardox® wear plate.

We also process parts with mechanical chamfering and grinding for edge preparation.

Steel plates.

The right materials for the job

We are experts in the processing of high-strength and special steels, like Strenx® performance steel, Hardox® wear plate, SSAB Domex®, Docol®, SSAB Laser® or SSAB Multisteel.

Contact us