Custom steel processing for OEMs and end-users

At SSAB Steel Service Center Montreal, we are experts in best practices for cutting, drilling, machining, and welding Hardox® wear plate, Strenx® structural steel, and Duroxite® overlay to your exacting OEM specifications.

For upgraded retrofit solutions, we use FARO 3D measurement, imaging, and realization technology to guide our CAD department in developing exacting designs for guaranteed fit and function.

Our manufacturing facility is certified to ISO 9001 and CWB 47.1 standards.

Oxyfuel/Plasma cutting

TABLE SIZE: 10’ x 50’ (3 x 15m)
1 PLASMA HEAD: cuts from 1/8” to 1-1/2” (3 to 38mm) thick plates
5 OXYFUEL HEADS: cut from ¾” to 5” (19 to 127mm) thick plates
Underwater cutting available

Plasma cutting

TABLE SIZE: 10’ x 50’ (3 x 15m) for dry cutting
2 PLASMA HEADS: cut from 1/8” to 1-1/4” (3 to 31mm) thick plates

Fiber laser

5-Axis Plasma, 2-Axis Oxyfuel, and Machining Center

TABLE SIZE: 10’ x 50’ (3 x 15m) for dry cutting
1 PLASMA HEAD: cuts from 1/8” to 2” (3 to 50mm) thick plates
3 OXYFUEL HEADS: cut from 2” to 6” (50 to 152mm) thick plates
MACHINING: from 3/8” to 6” (9.5 to 152mm) thick plates

Waterjet machine with 5-Axis Cutting Head

TABLE SIZE: 10’ x 26’ (3 x 7.9m)
2 HEADS: cut from 0.164” to 4-1/2” (4.16 to 114mm)

Laser cutting

Fiber Laser, 6kW

TABLE SIZE: 8’ x 60’ (2.4 to 18.3m)
LASER: cuts 0.0787” to 0.5” (2 to 12.7mm)

welding

Welding

MIG/FCAW/SMAW processes
Stud welding
Hardfacing: Duroxite® and tungsten overlays
3rd party certification to CWB 47.1 standards for welders, welding supervisors and engineers, and welding procedures.

CNC machining center

TABLE SIZE: 47.2’’ x 118’’ (3000mm x 1100mm)
Double column machining center - 3 axis

The right steel for each equipment

Which SSAB steel are right for your component?

Contact us

Get us involved as early for the best possible outcomes on your project — whether you are upgrading existing equipment or doing bold, innovative OEM designs. We’ll help your steel equipment become lighter, more wear resistant, and longer lasting.