    General Product Description

    The ballistic protection steel with extra-high hardness.

    Ramor® 550 is a ballistic protection steel of extra-high hardness, available in thicknesses of 3.0 ‑ 15.0 mm (0.118‑0.591″) and hardnesses of 540‑600 HBW.

    Ramor® 550 is available as cut-to-length sheet in thicknesses of 3.0 ‑ 6.0 mm (0.118‑0.236″) and as plate in thicknesses of 6.0 ‑ 15.0 mm (0.236‑0.591″). Delivered in quenched condition, Ramor® 550 is not intended for further heat treatment.

    Mechanical Properties

    Hide/Show specific columns Edit
    Select columns to display
      Thickness
      (mm)
      Hardness
      (HBW)
      Ramor® 550 3.0 - 15.0 540 - 600
      Compare parameters

      Select one parameter to compare

      Comparison

        Mechanical Testing

        Brinell hardness test according to EN ISO 6506-1 on each heat treatment individual/coil.

        Hardness is measured on a milled surface 0.3-2 mm below plate surface.

        Chemical Composition (ladle analysis)

        Hide/Show specific columns Edit
        Select columns to display
          C
          (max %)
          Si
          (max %)
          Mn
          (max %)
          P
          (max %)
          S
          (max %)
          Cr
          (max %)
          Ni
          (max %)
          Mo
          (max %)
          B
          (max %)
          0.36 0.70 1.5 0.015 0.010 1.50 2.50 0.80 0.005
          Compare parameters

          Select one parameter to compare

          Comparison

            The steel is grain-refined. Phosphorous and sulphur are not intentionally alloying elements.

            Tolerances

            More details are given on www.ssab.com.

            Thickness

            Hide/Show specific columns Edit
            Select columns to display
              Product Type Thickness
              (mm)
              Tolerance
              (mm)
              Sheet 3.00 - 4.00 - 0.0 / + 0.36
              Sheet 4.01 - 5.00 - 0.0 / + 0.40
              Sheet 5.01 - 6.00 - 0.0 / + 0.42
              Plate 6.0 - 7.9 - 0.0 / + 0.8
              Plate 8.0 - 15.0 - 0.0 / + 1.0
              Compare parameters

              Select one parameter to compare

              Comparison

                Length and Width

                Sheets are delivered with mill edges cut as standard.

                • Tolerances conform to EN 10 051 or to SSAB´s standard after agreement.

                Plate delivered according to SSAB’s dimension program.

                • Tolerances conform to EN 10 029 or to SSAB’s standard after agreement.
                • Dimensional tolerances for plate with mill edge according to special agreement. 

                Shape

                Tolerances according to EN 10029 for plate and according to EN 10051 for sheet.

                Flatness

                Tolerances according to SSAB’s flatness tolerances which are more restrictive than EN 10 029 Class N (steel type L) and EN 10 051.

                Hide/Show specific columns Edit
                Select columns to display
                  Product Type 1000 ruler
                  (mm)
                  Sheet 6
                  Plate 6
                  Compare parameters

                  Select one parameter to compare

                  Comparison

                    Surface Properties

                    According to EN 10163-2 Class B Subclass 3.

                    Delivery Conditions

                    Ramor is delivered in quenched condition.