The welding process subjects a joint to a localized thermal heat treatment.

This effect contributes to that the joint attains different mechanical properties and microstructures compared to that of the unaffected parent metal. The mechanical properties that are mostly affected by the thermal cycle are toughness, static strength and hardness values in the joint.

Welding properties are of vital concern for SSAB during the development of our steels. As a result, these steels can achieve favorable properties in the joint. This is achieved by following the welding recommendations stated by SSAB.

The complete part of the parent metal that is influenced by the thermal cycle from welding is called the heat affected zone (HAZ). The other main areas in the joint are the unaffected parent metal and the weld metal, see illustrations below.

The principal parts of the joint: a) Unaffected parent metal. b) Heat affected zone, HAZ. c) Weld metal.

Contact Technical support


The information in this report is only applicable to SSAB’s products and should not be applied to any other products than original SSAB products. 


This report provides general results and recommendations for SSAB steel products. This report is subject to SSAB’s Terms of Use. It shall be the user's responsibility to verify that the information contained herein is correct and is suitable to be used for the particular purpose and application of the user. The report is intended to be used by professional users only who possess adequate expertise, qualification and knowledge for the safe and correct use of the results and recommendations in this report. This report is provided “as is”. The use of the report is at user’s own discretion and risk and that users will be solely responsible for any use of this report. SSAB disclaims any liability for the content or potential errors of this report, including but not limited to warranties and condition of merchantability or fitness for a particular purpose or suitability for individual applications. SSAB shall not be liable for any kind of direct or indirect damages and/or costs related to or arising therefrom, whether special, incidental, consequential or directly or indirectly related to the use of, or the inability to use, the report or the content, information or results included therein. 

Copyright 2026