SSAB Form comes in a wide range of grades, making it easier for you to optimize your production and the performance of the final product. SSAB Form is delivered as hot rolled strip, cold rolled strip, metal-coated grades, and tubes. Delivery condition can be with or without anti-corrosion surface protection.
SSAB Form metal-coated grades for corrosion resistance are available with zinc, galfan, and galvannealed coatings. Zinc coating by hot-dip galvanizing up to 42 μm on both sides can give service life of up to 80 years. Galfan grades give excellent corrosion resistance, weldability, and formability with a thinner 7-23 μm zinc-aluminum coating. Galvannealed grades have a 6-10 μm zinc-iron alloy-coating ideal for spot welding and high-end painting applications.
You can order a wide range of plates, tubes and sections of SSAB Form from our stock network or straight from mill. Smaller volumes are also available to suit your production and storage capacity.
Your local SSAB contact will answer any questions about ordering and shipping, delivery times, marking and packing.
SSAB Form 200 Hot-rolled
SSAB Form 200 Cold rolled
SSAB Form 03
SSAB Form 04
SSAB Form 05
SSAB Form 06
SSAB Form 07
SSAB Form 200 Metal coated
SSAB Form 52
SSAB Form 53
SSAB Form 54
SSAB Form 56
SSAB Form 57
SSAB Form TSP
SSAB Form PLX
SSAB Form Tube 220
SSAB Form Tube 320