SSAB Boron and SSAB M53 steels come in a wide range of steel grades with carbon contents from 0.22–0.535 %. Available as hot rolled plate, hot rolled coil; slit coil and sheet; cold rolled coil, slit coil and sheet; tubes and sections. Hot rolled strip products are available in black, pickled and annealed condition. Availability is depended on grade. Tubes and sections are produced from hot and cold rolled base material.

*The hardness values in the diagram are indicative. Composition, hardness measurement depth, austenitizing temperature and time, hardening process and material thickness are affecting to the final hardness.
In order to suit your production and logistic preferences, SSAB Boron can be sourced directly from our mills or through our stocks. Please consult your local SSAB contact to design the optimal delivery solution for you.
Contact usSSAB Boron 22
SSAB Boron 24
SSAB Boron 27
SSAB Boron 27Cr
SSAB Boron 30
SSAB Boron 33
SSAB Boron 33Cr
SSAB Boron 36
SSAB Boron 38
SSAB Boron 42
SSAB Boron 45