SSAB Zero™ is made using recycled steel and fossil-free electricity, biocoal and biofuels. It reduces the embeded CO2e emissions from the steel by up to 70% compared to hot-rolled steel made in SSAB’s blast furnace production system. Without compromising on quality or performance, SSAB Zero™ helps lower the carbon footprint of your construction and manufacturing projects.
Our EPDs (Environmental Product Declarations), provide third-party-verified data on the environmental impact of SSAB Zero™. They enable you to communicate about the sustainable performance of your products.
The chart shows the CO2e reductions of SSAB Zero™ steel compared with SSAB’s traditional blast furnace steel (BF 2025).

GWP Modules A1–A3, cradle to gate.
* SSAB Zero™ Tubes and profiles EPDs to be updated in H2/2026.
The emission values 0.57 and <0.05 kg CO2e/kg steel measure different aspects of the production process. They are both third-party verified by recognized institutions, ensuring transparency and credibility.





Join us for an inspiring webinar, where we present the new EPDs that are now available for SSAB Zero™.
Topics we will go through during this webinar:

This webinar is available in English, Swedish, Finnish, Spanish and French:

Keep the same exceptional performance and properties while saving CO2. Our list of high-quality SSAB Zero™ steel products is growing continuously for easy conversion from your current steel.

SSAB Zero™ enables sustainable performance, delivering the same top quality and all other requirements you would expect from SSAB. Learn more about products made with less CO2 emissions.
Why our customers are using SSAB Zero™ in their products