SSAB AM Engineering

Download data sheet

Select Language

Get datasheet by email
Close

Get datasheet by email

On this page

General Product Description

SSAB AM Engineering is a gas atomised low-alloyed powder for additive manufacturing of high strength engineering components. SSAB AM Engineering is in particular suited in L-PBF (Laser-Powder Bed Fusion) and Direct Energy Deposition (DED or LMD).

The spherical powder enables an optimal combination of strength, toughness and high levels of isotropy in the as-built condition.

SSAB AM Engineering is a steel grade with low CO2 emissions and planned for Zero™ and fossil-free properties (see www.ssab.com/fossilfree).

Powder Properties

Standard particle size distribution.

Hide/Show specific columns Edit
Select columns to display
    L-PBF 20 - 53 µm 1)
    DED 45 - 106 µm 1)
    Compare parameters

    Select one parameter to compare

    Comparison

      L-PBF
      20 - 53 µm 1)
      DED
      45 - 106 µm 1)

      1) Max 5% over and under size.

      Measurement of particle size distribution is according to ISO 13322-2 (Dynamic image analysis methods).

      Other particle size distributions can be arranged upon agreement.

      Generic Data

      Achievable generic data in as-built parts: L-PBF

      Hide/Show specific columns Edit
      Select columns to display
        Density 7.8 g/cm3
        Young´s Modulus 200 GPa
        Compare parameters

        Select one parameter to compare

        Comparison

          Density
          7.8 g/cm3
          Young´s Modulus
          200 GPa

          Physical Properties

          Hide/Show specific columns Edit
          Select columns to display
            Heat conductivity (W/m*K) Thermal expansion coefficient (10-6/K)
            +20 °C 30 13
            +200 °C 34 15
            +400 °C 35 14
            Compare parameters

            Select one parameter to compare

            Comparison

              Mechanical Properties

              Achievable mechanical properties in as-built parts: L-PBF

              Hide/Show specific columns Edit
              Select columns to display
                Product Hardness
                (HV5)
                Tensile strength
                (MPa)
                Yield strength
                (MPa)
                Elongation A5
                (%)
                Impact toughness (Charpy V)
                at RT 1)/ at -40 oC
                SSAB AM Engineering 340 1240 1140 14 140 J / >47 J
                Compare parameters

                Select one parameter to compare

                Comparison

                  1) At room temperature.

                  All test samples have been produced on a SLM 280 2.0 system, 30 µm layer thickness and tested in the vertical direction.

                  Chemical Composition (heat analysis)

                  Hide/Show specific columns Edit
                  Select columns to display
                    C
                    (max %)
                    Si
                    (max %)
                    Mn
                    (max %)
                    Cr
                    (max %)
                    Mo
                    (max %)
                    Fe
                    0.26 1.5 1.0 1.5 0.4 Balance
                    Compare parameters

                    Select one parameter to compare

                    Comparison

                      Delivery Conditions

                      Standard package size for SSAB AM Engineering powder is 10 kg, including silica gel bag. Other package sizes are available up on agreement.

                      Safety Information Sheet