Maximize your choice of AHSS/UHSS automotive solutions: Docol® automotive steel grades include martensitic • press hardening steel • complex phase • high edge ductility • 3rd gen dual phase with high formability • and more. SSAB uses pure Swedish iron ore and advanced milling processes to make steels with extremely clean properties and highly consistent formability.
In addition to the automotive steel grades listed below, SSAB offers hundreds of Docol® variations to meet specific VDA, SAE, EN, JIS, and OEM standards. We work in close cooperation with automotive OEMs and Tier 1 suppliers to develop custom AHSS grades that give your designs a competitive edge.
Custom AHSS for automotive OEMs

We can help at each step: material selection, crash simulations, design optimization, production modeling, effective workflow planning, and tooling recommendations. Plus, you have immediate access to on-demand webinars and articles on key issues such as AHSS simulations, managing springback, and fossil-free automotive steel.
Docol resourcesIn addition to the open for sales steels listed in the “Available steel grades” tables below, SSAB is constantly developing new Docol® grades based on future needs of leading car OEMs and Tier 1 suppliers.
Here’s a list of exciting new AHSS developments. Some are “steel family extensions” — that is, grades now available in new hot-rolled or metal-coated versions. Others are all-new automotive metals, like our guaranteed hole-expansion ratio (HER) grades.
New hot-rolled grades:
Docol HR800HER-75
Docol HR1500M
Docol HR1000CP
New cold-rolled grades:
Docol 1900M
Docol 1700M-EG
New metal-coated grades:
Docol CR1180CP-GI
Docol CR1180DP-GI
Docol CR1000DH-GI
Docol HR600FB-GI
Martensitic (M) steels have very high yield strength (Re) and an extremely high tensile strength (Rm). Docol® martensitic steel has good draw ability and good edge stretching properties. It is also good in welding.
Docol® Martensitic phase steel product offer:
Docol 900M
Docol 1100M
Docol 1200M
Docol 1300M
Docol 1400M
Docol 1700M
*Available upon request.
Metal coated Docol® 600DH-GI and 800DH-GI are two of the steel grades now avaliable and more are on the way.
DA special heat treatment producing mainly two-phase structure makes Docol® 600DH-GI and 800DH-GI suitable where an improved formability is requested compared to conventional dual-phase steel grades with the same tensile strength level.
Docol 600DH
Docol 800DH
For Press Hardening (PHS) Steel it is the forming process which sets the final characteristics on the material. Forming at high temperatures facilitates complex structures as the martensitic microstructure is developed after press hardening. This material has a limitation in welding properties.
Docol® PHS steel product offer:
Docol PHS 1800
Docol PHS 1500
Complex Phase (CP) steels have higher yield strength and lower work hardening effect, compared to DP steels for same strength level. The CP steels have good fatigue properties when it comes to low cycle fatigue. Compared to DP, the CP steels offer better flanging and ISO hole expansion performance and these automotive metals are suitable for applications where high strength, good bendability and stretch-flange ability is required.
Docol 600CP
Docol 800CP
Docol 1000CP
Docol 1200CP
*Available upon request.
For Dual Phase (DP) steels there is a big difference in yield and tensile strength in un-deformed areas. The work hardening in forming is very strong. DP steels have good formability compared to its strength but are limited in hole expansion. With its lean composition these steels are easy to weld but sensitive to heat treatment (> 200 °C).
Docol® dual phase steel product offer:
Docol 500DP
Docol 800DP
Docol 1000DP
*Available upon request.
Docol® HE is a new range of hot rolled advanced high strength steel (AHSS) with improved edge ductility for automotive manufacturers facing technical challenges in production.
Docol® High Edge Ductility steel product offer:
Docol 355HE
Docol 420HE
Docol 460HE
Docol 500HE
Docol 550HE
High Strength Low Alloy (HSLA) steels have a typically small difference between yield strength and tensile strength (<100 MPa). They, therefore, offer excellent bendability. With little pearlite and no other hard phases they also have better fine blanking properties compared to DP steels and due to lean composition they are very easy to weld.
Docol® High Strength Low Alloy steel product offer:
Docol S600MC
Docol 500LA
Docol 420LA
Docol 550LA
Docol 600LA
Docol 650LA
Docol 700LA
Docol S900MC
Docol S960MC
Docol HR100XF
Docol HR110XF
*Available upon request.
Ferritic-Bainitic (FB) steels have mechanical properties that are similar to Complex Phase (CP) steels but with a higher gap between yield and tensile strength. FB steels are characterized by good bendability and excellent stretch-flange ability. They are best suited for parts with stretched flanges such as chassis components in cars.
Docol 600FB
*Available upon request.
Docol Tubes offer the market´s greatest strength range. The tensile strength range starts from 600 MPa and goes up to an extraordinary 1000 MPa without any post-heat treatments. With coating options including zinc, galfan and galvannealed, corrosion resistance and superior paint adhesion can be combined for the first time in high-strength precision tubing. Docol Tubes are made in compliance with standard EN 10305 (parts 3 and 5) with the more demanding elongation values and chemical analyses. To meet the highest customer expectations, we manufacture the tubes with narrow tolerances.
Docol Tube 590DP