General Product Description

GreenCoat Pural BT color coated steel is available in satin, regular and matt finishes and offers a wide range of colors inspired by Nordic nature. It uses a patented bio-based coating with Swedish rapeseed oil, which is unique on the market. SSAB holds a worldwide patent for this coating technology (Bio-based Technology, BT).

GreenCoat Pural BT offers the highest level of durability for roofing applications like standing seams, profiled roof tiles and is used widely in metal roofer applications. Besides the regular gloss GreenCoat Pural BT in non-metallic colors can be used in facade products like, sandwich panels and cassettes.

GreenCoat Pural BT color coated steel offers a coating that is optimized to resist weathering resulting in the highest UV (Ruv5 for matt appearance) and corrosion classes (RC5+). The slightly structured surface helps to protect against mechanical wear and is easy to handle during manufacturing. GreenCoat Pural BT possesses excellent forming properties enabling very demanding folding even down to -15°C, allowing for year round installation at lower costs.

The newly developed satin appearance of GreenCoat Pural BT responds well to current architectural and design trends. It has a gloss level of 20.

The reverse side of the sheet is painted with a two-layer grey backside coating.

GreenCoat Pural BT complies with current REACH regulations and is fully chromate-free.

SSAB’s color coated steels are all manufactured according to EN 10169.

GreenCoat and Pural are trademarks of the SSAB group of companies.

Technical Properties

Hide/Show specific columns Edit
Select columns to display
    Technical Properties Matt Regular Satin
    Gloss < 5 40 20
    Minimum inner bending radius 1 x sheet thickness 1 x sheet thickness 1 x sheet thickness
    Scratch resistance 40 N 40 N 40 N
    Lowest forming temperature -15 °C -15 °C -15 °C
    UV radiation resistance RUV5 RUV4 RUV4-5
    Corrosion resistance 1) RC5+ RC5+ RC5+
    Stain resistance Very good Very good Very good
    Highest operating temperature 100 °C 100 °C 100 °C
    Fire classification, EN 13501-1 A1 s1 d0 A1 s1 d0 A1 s1 d0
    Coating thickness, nominal (primer + top coat) 50 µm 50 µm 50 µm
    Coating structure Structured and wrinkled Structured Structured
    Steel designation 2) S280GD, S320GD, S350GD S280GD, S320GD, S350GD S280GD, S320GD, S350GD
    Zinc coating 275 g/m2 275 g/m2 275 g/m2
    Min steel thickness 2) 0.50 mm 0.50 mm 0.50 mm
    Steel width 2) 1000 - 1500 mm 1000 - 1500 mm 1000 - 1420 mm
    Compare parameters

    Select one parameter to compare

    Comparison

      1) Classification into corrosion resistance categories is based on blistering, delamination and damage on bend of the coating after four years exposure in natural outdoor testing sites as specified in EN 10169.

      2) Maximum steel thickness is 1.5 mm and maximum steel width depends on steel thickness. For other steel dimensions or steel grades please contact SSAB Tech Support.

      Colors

      Below are the colors currently available. Other colors can be agreed upon separately.

      Colors shown in the color table are only indicative. To see the real visual appearance of the product, please order a color sample. Please note also that the same colors between the products may differ.

      For information on thermal properties (solar reflectance index SRI or thermal emittance TE) of available colors, please contact SSAB Tech Support.

      29 Available Colors
      Preview colors
      Close

      Colors

      GreenCoat Pural BT

      Winter White

      RR20 / SS0005

      Regular, Matt

      Snow White

      RR19 / SS0001

      Matt

      Concrete Grey

      RR292 / SS----

      Regular

      Pebble Grey

      RR21 / SS0011

      Regular, Matt

      Quarry Grey

      RR287 / SS0244

      Regular, Matt

      Stone Grey

      RR22 / SS0554

      Regular, Matt, Satin (trial deliveries)

      Anthracite Grey

      RR2H8 / SS0087

      Matt

      Mountain Grey

      RR23 / SS0036

      Regular, Matt, Satin

      Ridge Grey

      RR2F7 / SS0035

      Regular

      Slate Grey

      RR2H3 / SS0534

      Regular, Matt

      Nordic Night Black

      RR33 / SS0015

      Regular, Matt, Satin

      Walnut Brown

      RR32 / SS0387

      Regular, Matt, Satin

      Chestnut Brown

      RR887 / SS0435

      Regular, Matt

      Almond Brown

      RR30 / SS0187

      Regular

      Terra Brown

      RR31 / SS0433

      Regular

      Cottage Red

      RR29 / SS0758

      Regular, Matt, Satin

      Tile Red

      RR750 / SS0760

      Regular, Matt, Satin (trial deliveries)

      Brick Red

      RR7F2 / SS0742

      Regular

      Wine Red

      RR798 / SS5781

      Regular, Matt

      Harvest Yellow

      RR24 / SS0189

      Regular

      Silver Fir Green

      RR5J3 / SS0975

      Matt

      Leaf Green

      RR594 / SS0874

      Matt

      Pine Green

      RR11 / SS0830

      Regular, Matt, Satin (trial deliveries)

      Green

      RR37 / SS0925

      Regular

      Lake Blue

      RR35 / SS0558

      Regular

      Metallic Silver

      RR40 / SS0045

      Regular

      Metallic Dark Silver

      RR41 / SS0044

      Regular, Matt

      Metallic Gold

      RR42 / SS----

      Regular

      Metallic Copper

      RR979 / SS0778

      Regular

      Note especially for Metallic and all Matt colors: To ensure tonal consistency of colors on a single exterior face, all material must come from the same production batch. Also the directionality of surfaces has to be consistent especially when sheets are cut to size. Compared to solid colors, larger measured color variation between production batches is typical for metallic colors, even if color is visually stable.

      Reverse Side Coating

      Unless otherwise specified, the reverse side of the sheet is painted with a two-layer coating to further improve the corrosion resistance of the end product. The coating provides good adhesion properties to many adhesives and foams; nevertheless the compatibility needs to be tested case-specifically.

      Hide/Show specific columns Edit
      Select columns to display
        Technical Properties
        Nominal Coating Thickness (primer + top coat) 12 µm
        Color Grey
        Corrosion Resistance Min CPI3
        Compare parameters

        Select one parameter to compare

        Comparison

          Technical Properties
          Nominal Coating Thickness (primer + top coat)
          12 µm
          Technical Properties
          Color
          Grey
          Technical Properties
          Corrosion Resistance
          Min CPI3

          For easy material identification the reverse side of the sheet is stamped with the GreenCoat logo and the product name. The production year is marked to ease material traceability and can be referred to within the guarantee period. An arrow shows the direction of production to ensure installation in a uniform direction.

          Contact Information