Tubes product group

Product Name

SSAB Domex Tube 355J2H

Dimensions
Circular: 42.4 - 323.9 mm
Square: 40x40 - 300x300 mm
Rectangular: 50x30 - 400x200 mm
Wall Thickness: 2.0 - 12.5 mm
Circular: 1.67 - 12.75 in
Square: in
Rectangular: in
Wall Thickness: 0.079 - 0.492 in
Standards
EN 10219-1, EN 10219-2
Datasheet
Product Name

SSAB Domex Tube 460MH

Dimensions
Circular: 42.4 - 323.9 mm
Square: 40x40 - 300x300 mm
Rectangular: 50x30 - 400x200 mm
Wall Thickness: 2.0 - 12.5 mm
Circular: 1.67 - 12.75 in
Square: in
Rectangular: in
Wall Thickness: 0.079 - 0.492 in
Standards
EN 10219-1, EN 10219-2
Datasheet
Product Name

SSAB Domex Tube 500MH

Product Name

SSAB Domex Tube 550MH

Dimensions
Circular: 42.4 - 323.9 mm
Square: 40x40 - 300x300 mm
Rectangular: 50x30 - 400x200 mm
Wall Thickness: 2.0 - 12.50 mm
Circular: 1.67 - 12.75 in
Square: in
Rectangular: in
Wall Thickness: 0.079 - 0.4921 in
Standards
EN 10219-2, EN 1090-2
Datasheet
Copyright 2026