GreenCoat Mica BT

Download data sheet

General Product Description

GreenCoat Mica BT color coated steel is available in an exclusive, glittery matt textured finish. It provides a coating where rapeseed oil and other renewable raw materials are used. SSAB has long experience of Bio-based Technology (BT) in GreenCoat® products.

GreenCoat Mica BT color coated steel offers a high level of durability for profiled roof tiles and profiles with high aesthetic demands. GreenCoat Mica BT possesses good gloss retention and color fastness and provides good protection against corrosion (RC5 class). The reverse side of the sheet is painted with a two-layer grey backside coating.

GreenCoat Mica BT complies with current REACH regulations and is fully chromate-free.

SSAB’s color coated steels are all manufactured according to EN 10169.

Technical Properties

Technical Properties
Technical Properties
Gloss
Matt
5
Technical Properties
Technical Properties
Minimum inner bending radius
Matt
1.5 x sheet thickness
Technical Properties
Technical Properties
Scratch resistance
Matt
30 N
Technical Properties
Technical Properties
UV radiation resistance
Matt
RUV3
Technical Properties
Technical Properties
Corrosion resistance 1)
Matt
RC5
Technical Properties
Technical Properties
Stain resistance
Matt
Very good
Technical Properties
Technical Properties
Highest operating temperature
Matt
100 °C
Technical Properties
Technical Properties
Fire classification, EN 13501-1
Matt
A2 s1 d0
Technical Properties
Technical Properties
Coating thickness, nominal (primer + top coat)
Matt
30 µm
Technical Properties
Technical Properties
Coating structure
Matt
Wrinkled
Technical Properties
Technical Properties
Steel designation 2)
Matt
S280GD, S320GD, S350GD
Technical Properties
Technical Properties
Zinc coating
Matt
275 g/m2
Technical Properties
Technical Properties
Min steel thickness 2)
Matt
0.50 mm
Technical Properties
Technical Properties
Steel width 2)
Matt
1000 - 1500 mm

1) Classification into corrosion resistance categories is based on blistering, delamination and damage on bend of the coating after two years exposure in natural outdoor testing sites as specified in EN 10169.

2) Maximum steel thickness is 1.5 mm and maximum steel width depends on steel thickness. For other steel dimensions or steel grades please contact SSAB Tech Support.

Colors

Below are the colors currently available. Other colors can be agreed upon separately.

Colors shown in the color table are only indicative. To see the real visual appearance of the product, please order a color sample. Please note also that the same colors between the products may differ.

To ensure tonal consistency of colors on a single exterior face, all material must come from the same production batch. Also the directionality of surfaces has to be consistent especially when sheets are cut to size.

Reverse Side Coating

Unless otherwise specified, the reverse side of the sheet is painted with a two-layer coating to further improve the corrosion resistance of the end product. The coating provides good adhesion properties to many adhesives and foams; nevertheless the compatibility needs to be tested case-specifically.

Technical Properties
Technical Properties
Nominal Coating Thickness (primer + top coat)
12 µm
Technical Properties
Technical Properties
Color
Grey
Technical Properties
Technical Properties
Corrosion Resistance
Min CPI3

For easy material identification the reverse side of the sheet is stamped with the GreenCoat logo and the product name. The production date is marked to ease material traceability and can be referred to within the guarantee period. An arrow shows the direction of production to ensure installation in a uniform direction.