The ballistic protection steel with extra-high hardness
Ramor® 600 is a ballistic protection steel of extra-high hardness, nominal 600 HBW, available in thicknesses of 3.0 ‑6.0 mm (0.118‑0.236″).
Ramor® 600 is available as cut-to-length sheet in thicknesses of 3.0 ‑ 6.0 mm (0.118‑0.236″). Delivered in quenched condition, Ramor® 600 is not intended for further heat treatment.
Thickness (mmin) | Hardness (HBW) | |
|---|---|---|
Ramor® 600 | 3.0 - 6.00.118 - 0.236 | 570 - 640 |
Ramor® 600
Brinell hardness test according to EN ISO 6506-1 on each heat treatment individual/coil.
Hardness is measured on a milled surface 0.3-2 mm below plate surface.
C (max %) | Si (max %) | Mn (max %) | P (max %) | S (max %) | Cr (max %) | Ni (max %) | Mo (max %) | B (max %) |
|---|---|---|---|---|---|---|---|---|
0.40 | 0.70 | 1.5 | 0.015 | 0.010 | 1.50 | 2.50 | 0.80 | 0.005 |
The steel is grain refined. Phosphorous and sulphur are not intentionally alloying elements.
More details are given on www.ssab.com.
Product Type | Thickness (mmin) | Tolerance (mmin) |
|---|---|---|
Sheet | 3.00 - 4.000.118 - 0.157 | - 0.0 / + 0.36- 0.0 / + 0.0142 |
Sheet | 4.01 - 5.000.158 - 0.197 | - 0.0 / + 0.40- 0.0 / + 0.0157 |
Sheet | 5.01 - 6.000.198 - 0.236 | - 0.0 / + 0.42- 0.0 / + 0.0165 |
Sheets are delivered with mill edges cut as standard.
Tolerances according to EN 10051.
Tolerances according to SSAB’s flatness tolerances which are more restrictive than EN 10051.
Product Type | 1000 ruler (mmin) |
|---|---|
Sheet | 60.236 |
According to EN 10163-2 Class B, Subclass 3.
Ramor® is delivered in quenched condition.