Docol Tube 780DP

Docol® Tube 780DP

Provides a balanced combination of high strength and formability

Docol® Tube 780DP is advance high-strength formable precision tube made from dual-phase steel with high tensile strength, improved formability or enhanced proofed yield strength. Available in circular, rectangular and square shapes, it comes with different coating and surface options including cold rolled (uncoated), galvanized, galvannealed and galfan. Customized shapes and other tailoring options are available upon request. Typically used in automotive industry where durability, formability and energy absorption are important. 

Docol® Tube 780DP is manufactured by cold forming and high-frequency welding from clean, high-quality SSAB steel by modern and efficient tube lines.

Dimension Range

Docol Tube 780DP is available at circular, square and rectangular shapes. 

   
Circular 16 - 76 mm 
Square 19x19 - 60x60 mm 
Rectangular 20x15 - 80x40 mm 
Wall thickness 1.0 - 2.0 mm
Mill length 6000 mm

Other shapes, sizes and lengths are available upon request.

Available Standards

EN 10305-3

EN 10305-5

VDA 239-100:2016