Transformation roadmap

SSAB’s Board of Directors took the decision to invest SEK 6.2 billion in an electric arc furnace (EAF) in Oxelösund in June 2023. This was the starting point of the transformation of the Nordic production system. With regard to the mini-mill in Luleå, the decision to invest was taken in April 2024. The third step in the transformation is the planned transformation of Raahe. The timing of the Raahe project will depend on SSAB’s financing and implementation capacity, raw material availability and the lessons learned from the Luleå project. SSAB Americas plays an important role in the transformation, providing unique knowledge and experience from EAF steelmaking. SSAB Americas has been spearheading SSAB Zero™, introduced in the market in 2023.

Green and sustainability-linked finance

In 2024, SSAB launched a new combined Green and Sustainability-Linked Finance Framework that provides us with an opportunity to issue both green and sustainability-linked financing instruments, as well as a combination of the two.

This means we are taking a pivotal step in our transformation toward fossil-free steelmaking and reduced carbon dioxide emissions. The framework contains ambitious, science-based emission reduction targets and sets clear guidelines for our green investments.

Shipments of decarbonized steels

The production of fossil-free steel has already started as a proof of concept and test batches have been shipped to strategic partners since 2022. In 2023, our new SSAB Zero™ steel produced in Iowa, USA, was introduced. When transforming our Nordic sites, we will benefit from our experience from the USA, where we use EAFs in steel production at our sites in Montpelier and Mobile. This includes the most advanced quenched and tempered (Q&T) grades.

Key performance improvements

The transformation will increase the capacity for premium products, improve our cost position, shorten lead times and enable fossil-free steelmaking. The plan is to transform the Luleå mill into a new cost-effective mini-mill, with electric arc furnaces, integrated rolling and further processing and to replace the blast furnaces in Raahe with electric arc furnaces in the same way as in Oxelösund. The sites in Borlänge and Hämeenlinna will be further developed in line with the new production processes.

Sites well suited for a new future

The present production sites have great advantages for the future. The sites are large, which means that it will be possible to run old and new systems in parallel during the transition period. Important logistics capabilities exist from the start, with direct access to harbors, railway and road transports as well as raw material handling capabilities.

Luleå

  • Blast furnace-based steel production
  • Crude steel production capacity: 2.3 million tonnes
  • Employees: 1,200
  • Established: 1941

Oxelösund

  • Blast furnace-based steel production, heavy plate
  • Crude steel production capacity: 1.5 million tonnes
  • Employees: 2,400
  • Established: 1913

Borlänge

  • Strip products
  • Employees: 1,800
  • Established: 1878

Raahe

  • Blast furnace-based steel production, heavy plate and strip products
  • Crude steel production capacity: 2.6 million tonnes
  • Employees: 2,600
  • Established: 1960

Hämeenlinna

  • Strip and tubular products
  • Employees: 1,000
  • Established: 1972

Montpelier and Mobile

  • Scrap based electric arc furnace steel production, heavy plate
  • Employees: 650 in Mobile, Alabama and 450 in Montpelier, Iowa
  • Annual steel production capacity: approx 2.5 million tonnes (1.29 respectively)
  • Both SSAB Alabama and SSAB Iowa were constructed and opened by IPSCO, acquired by SSAB in 2007. Alabama opened in 2001 and Iowa opened in 1997.

Other press releasesSSAB and partners launch closed loop steel recycling initiative in the U.S.
Sustainability, SSAB Americas, Fossil-free steel, SSAB Zero
Other press releasesBusiness Finland grants significant support to SSAB’s Sustainable World through Steels research and development program
Research and development, Fossil-free steel
Other press releasesSSAB and Rheinmetall sign agreement for fossil-free steel deliveries
Fossil-free steel, SSAB Zero