Docol Tube 700LA

Docol® Tube 700LA

Provides a combination of high strength and formability

Docol® Tube 700LA is a modern high-strength low-alloy precision tube with hot rolled pickled surface condition. Available in circular shape. Rectangular, square and customized shapes and other tailoring options are available upon request. Typically used in automotive industry where durability, lightness and consistent properties are important.

Docol® Tube 700LA is manufactured by cold forming and high-frequency welding from clean, high-quality SSAB steel by modern and efficient tube lines.

Dimension Range

Docol Tube 700LA is available at circular shapes. 

   
Circular 32 - 88.9 mm 
Wall thickness 2.0 - 3.0 mm
Mill length 6000 mm

Other shapes, sizes and lengths are available upon request.

Available Standards

EN 10305-3