How to cut > How to minimize distortions from thermal cutting

Reasons for distortions from thermal cutting

All thermal cutting methods apply heat to the material, causing it to expand. While steels generally have similar thermal expansion coefficients, high tensile steels tend to distort more severely than mild steel due to their increased resistance to yielding.

If heating is done in a small area and the expansion of this area is restricted by surrounding material, the material will distort or warp. Steels with lower strength may allow some stresses to be relieved through material yielding, whereas high-strength steels are more resistant to yielding, resulting in more severe deformations. 

When heating is done in a small area and the expansion is restricted by surrounding material, distortion or warping occurs. Steels with lower strength may allow some stresses to be relieved through material yielding, whereas high-strength steels are more resistant to yielding, resulting in more severe deformations.

Thicker materials tend to distort less because their stiffness makes them more resistant to deformation.

Contact Technical support


The information in this report is only applicable to SSAB’s products and should not be applied to any other products than original SSAB products. 


This report provides general results and recommendations for SSAB steel products. This report is subject to SSAB’s Terms of Use. It shall be the user's responsibility to verify that the information contained herein is correct and is suitable to be used for the particular purpose and application of the user. The report is intended to be used by professional users only who possess adequate expertise, qualification and knowledge for the safe and correct use of the results and recommendations in this report. This report is provided “as is”. The use of the report is at user’s own discretion and risk and that users will be solely responsible for any use of this report. SSAB disclaims any liability for the content or potential errors of this report, including but not limited to warranties and condition of merchantability or fitness for a particular purpose or suitability for individual applications. SSAB shall not be liable for any kind of direct or indirect damages and/or costs related to or arising therefrom, whether special, incidental, consequential or directly or indirectly related to the use of, or the inability to use, the report or the content, information or results included therein.