    General Product Description

    Duroxite® 101 is manufactured by depositing a chromium-rich carbide overlay on Hardox 450 backing plate. The hardfacing overlay is suitable for severe abrasive wear and impact applications. With its optimum carbide concentration, consistently good wear resistance from top surface through 75% depth of overlay, and Hardox backing plate, Duroxite® 101 provides a better combination of wear and impact resistance compared to the traditional mild steel backing overlay plate.

    Key Benefits

    • Designed to better withstand plastic deformation due to its high yield strength flexing back after impact
    • Stronger support due to high hardness of Hardox and better bonding between overlay and base steel
    • When overlay wears off Hardox® 450 backing plate will wear at a lower rate than mild steel providing a greater safety margin
    • Better performance for impact situations than Duroxite® 100 at elevated temperatures up to 350° C (660° F), but impact resistance is best at room temperature

    Typical Applications

    Duroxite® 101 is widely used in the mining, cement and power generation industries. Some specific applications include:

    Hide/Show specific columns Edit
    Select columns to display
      Mining Loader bucket liners, bucket lip and side shrouds, jaw shrouds
      Cement Heel pads and dewatering conveyors
      Power Coal discharger chutes
      Compare parameters

      Select one parameter to compare

      Comparison

        Mining
        Loader bucket liners, bucket lip and side shrouds, jaw shrouds
        Cement
        Heel pads and dewatering conveyors
        Power
        Coal discharger chutes

        For more information on applications see the Duroxite® Product brochure.

        Available Dimensions

        Hide/Show specific columns Edit
        Select columns to display
          Standard overlay thicknesses
          Metric unit
          6 mm on 6 mm
          10 mm on 10 mm
          12 mm on 12 mm
          6 mm on 20 mm
          6 mm on 25 mm
          6 mm on 32 mm
          Compare parameters

          Select one parameter to compare

          Comparison

            Standard overlay thicknesses

            Metric unit
            6 mm on 6 mm
            Standard overlay thicknesses

            Metric unit
            10 mm on 10 mm
            Standard overlay thicknesses

            Metric unit
            12 mm on 12 mm
            Standard overlay thicknesses

            Metric unit
            6 mm on 20 mm
            Standard overlay thicknesses

            Metric unit
            6 mm on 25 mm
            Standard overlay thicknesses

            Metric unit
            6 mm on 32 mm

            Other plate sizes and custom thicknesses can be produced upon request.

            Standard plate sizes

            Hide/Show specific columns Edit
            Select columns to display
              Metric unit Imperial Unite
              0.6 m x 1.15 m 23’’ x 45’’
              1.2 m x 2.4 m 4" x 8"
              1.4 m x 3.0 m 4.6" x 10"
              1.5 m x 3.0 m 5" x 10"
              1.8 m x 3.0 m 6" x 10"
              Compare parameters

              Select one parameter to compare

              Comparison

                Metric unit
                0.6 m x 1.15 m
                Imperial Unite
                23’’ x 45’’
                Metric unit
                1.2 m x 2.4 m
                Imperial Unite
                4" x 8"
                Metric unit
                1.4 m x 3.0 m
                Imperial Unite
                4.6" x 10"
                Metric unit
                1.5 m x 3.0 m
                Imperial Unite
                5" x 10"
                Metric unit
                1.8 m x 3.0 m
                Imperial Unite
                6" x 10"

                Other plate sizes and custom thicknesses can be produced upon request.

                Mechanical Properties

                Hide/Show specific columns Edit
                Select columns to display
                  Wear properties
                  ASTM G65 – Procedure A weight loss 2)
                  Number of overlay passes Typical surface hardness1)

                  (HRC)
                  Typical surface hardness1)

                  (HV)
                  Surface
                  (g max)
                  75 % depth of overlay 3)
                  (g max)
                  Multiple passes 59 - 62 675 - 750 0.18 0.18
                  Compare parameters

                  Select one parameter to compare

                  Comparison

                    1) Surface hardness is measured on machined flat surface just below overlay surface.

                    2) ASTM G65 - Procedure A weight loss, is a standard test measuring sliding abrasion resistance using a dry sand/rubber wheel apparatus. ASTM G65-Procedure A is the most severe test method.

                    3) ASTM G65 - Procedure A weight loss, wear test is conducted at 75% depth of the overlay materials to ensure consistently good wear resistance from the top surface through to the depth of 75% of the overlay.

                    Microstructure

                    The typical overlay microstructure of Duroxite® 101 is composed of a high proportion of extremely hard primary M7C3 chromium-rich carbides with a typical hardness of 1700 HK4) dispersed evenly in a ductile eutectic austenite matrix. The volume fraction of primary carbides is maintained between 30 to 50 % to provide a good combination of wear resistance and homogenous bonding.

                    4) HK is the Knoop microhardness which is primarily used for very brittle materials.

                    Tolerances

                    Thickness

                    Overall and overlay thickness tolerances can be guaranteed within ±10% of specified thickness.

                    Flatness

                    Plate flatness tolerance can be guaranteed within ±3 mm (±1/8”) over 1.5 m (5’) plate length for plate dimensions equal to or less than 1.5 m (5’) x 3.0 m (10’). For plates greater than 1.5 m (5’) wide by 3.0 m (10’) long, the following flatness guarantees apply.

                    Hide/Show specific columns Edit
                    Select columns to display
                      Standard overlay thicknesses
                      Flatness tolerance over 1.5 m plate length,
                      Metric unit
                      Metric unit 1.8 m x 3.0 m 2.4 m x 3.0 m
                      5 mm on 8 mm 32 41
                      6 mm on 6 mm 32 41
                      10 mm on 10 mm 19 25
                      12 mm on 12 mm 12 12
                      Compare parameters

                      Select one parameter to compare

                      Comparison

                        Delivery Conditions

                        Duroxite® 101 is normally supplied in an as-welded condition, but can also be supplied in a ground condition upon request.

                        Fabrication and Other Recommendations

                        Welding, cutting, forming and machining

                        Recommendations can be found in the Duroxite® Products brochure, or consult your local technical support representative.

                        Safety precautions

                        When welding or cutting Duroxite® products, smoke is produced containing harmful fumes and gases that are chemically highly complex and difficult to easily classify. The major toxic component in the fumes and gases produced in the process is hexavalent chromium. The proper exhaust ventilation equipment and fume-extraction torches are recommended, as well as suitable protective clothing and respiratory protection for operators.