    Strenx® 700

    Strenx® 700 is a group of structural steels with a minimum yield strengths between 650 and 700 MPa (94-101 ksi) depending on thickness.

    Hide/Show specific columns Edit
    Select columns to display
      Product Name Thickness range (mminches) Yield strength (min MPaksi) Standards Datasheet
      Strenx® 700 CR 0.7 - 2.10.03 - 0.083 700101 SSAB Specification

      Strenx® 700 CR

      Strenx® 700 E/F 4.0 - 160.00.157 - 6.299 650 - 70094 - 101 EN 10025-6

      Strenx® 700 E/F

      Strenx® 700 OME 4.0 - 130.00.157 - 5.118 700101 EN 10025-6

      Strenx® 700 OME

      Strenx® 700MC D/E 2.00 - 10.000.079 - 0.393 700101 EN 10149-2

      Strenx® 700MC

      Strenx® 700MC Plus 3.00 - 12.000.118 - 0.472 700101 EN 10149-2

      Strenx® 700MC Plus

      Strenx® P700 4.0 - 100.00.157 - 3.937 670 - 70097 - 101 EN 10028-6

      Strenx® P700

      Compare parameters

      Select one parameter to compare

      Comparison

        Strenx® 900

        Strenx® 900 is a group of high-strength structural steel grades with a minimum yield strengths between 830 and 900 MPa (120 - 130 ksi), making them an excellent choice for transportation and lifting devices.

        Hide/Show specific columns Edit
        Select columns to display
          Product Name Thickness range (mminches) Yield strength (min MPaksi) Standards Datasheet
          Strenx® 900 E/F 4.0 - 120.00.157 - 4.724 830 - 900120 - 130 EN 10025-6

          Strenx® 900 E/F

          Strenx® 900MC 3.00 - 10.000.118 - 0.393 900130 EN 10149-2

          Strenx® 900MC

          Strenx® 900 Plus 2.0 - 8.00.079 - 0.315 900130 EN 10025-6

          Strenx® 900 Plus

          Compare parameters

          Select one parameter to compare

          Comparison

            Strenx® 960

            Strenx® 960 is a group of high-strength structural steel grades with a minimum yield strengths between 850 of 960 MPa (123-139 ksi), making them an excellent choice for transportation and lifting devices.

            Hide/Show specific columns Edit
            Select columns to display
              Product Name Thickness range (mminches) Yield strength (min MPaksi) Standards Datasheet
              Strenx® 960 E/F 4.0 - 120.00.157 - 4.724 850 - 960123 - 139 EN 10025-6

              Strenx® 960 E/F

              Strenx® 960MC 3.00 - 10.000.118 - 0.393 960139 EN 10149-2

              Strenx® 960MC

              Strenx® 960 Plus 2.00 - 8.000.079 - 0.315 960139 EN 10025-6

              Strenx® 960 Plus

              Strenx® 960 CR 0.8 - 2.10.03 - 0.083 960139 SSAB Specification

              Strenx® 960 CR

              Compare parameters

              Select one parameter to compare

              Comparison

                Strenx® 1100

                Strenx® 1100 is a group of structural steel grades with a minimum yield strength of 1100 MPa (160 ksi). Excellent for advanced lifting devices.

                Hide/Show specific columns Edit
                Select columns to display
                  Product Name Thickness range (mminches) Yield strength (min MPaksi) Standards Datasheet
                  Strenx® 1100 Plus 4.00 - 8.000.157 - 0.315 1100160 SSAB Specification

                  Strenx® 1100 Plus

                  Strenx® 1100 E/F 4.0 - 40.00.157 - 1.575 1100160 SSAB Specification

                  Strenx® 1100 E/F

                  Strenx® 1100MC 3.00 - 8.000.118 - 0.315 1100160 EN 10149-2

                  Strenx® 1100MC

                  Strenx® 1100 CR 0.8 - 2.10.03 - 0.083 1100160 SSAB Specification

                  Strenx® 1100 CR

                  Compare parameters

                  Select one parameter to compare

                  Comparison

                    Strenx® 1300

                    Strenx® 1300 is a group of structural steel grades with a minimum yield strength of 1300 MPa (188 ksi). Excellent for advanced lifting devices.

                    Hide/Show specific columns Edit
                    Select columns to display
                      Product Name Thickness range (mminches) Yield strength (min MPaksi) Standards Datasheet
                      Strenx® 1300 E/F 4.0 - 15.00.157 - 0.591 1300188 SSAB Specification

                      Strenx® 1300

                      Compare parameters

                      Select one parameter to compare

                      Comparison

                        Strenx® 100/110

                        The high-strength, high-performance steel with a minimum yield strength of 100 ksi.

                        Hide/Show specific columns Edit
                        Select columns to display
                          Product Name Thickness range (inches) Yield strength (min ksi) Standards Datasheet
                          Strenx® 100 0.1875 - 5 94 - 100 ASTM A514
                          Strenx® 100XF 0.079 - 0.393 100 SSAB Specification
                          Strenx® 110XF 0.079 - 0.393 110 ASTM A1011/A1018 on request
                          Compare parameters

                          Select one parameter to compare

                          Comparison

                            Strenx® Tubes

                            Strenx® Tubes are tubes that combine high strength with a naturally stiff welded hollow section, enabling you to build stronger and lighter structures.

                            Hide/Show specific columns Edit
                            Select columns to display
                              Product Name Thickness range (mminches) Circular (mminches) Square (mminches) Rectangular (mminches) Yield strength (min MPaksi) Shapes Standards Datasheet
                              Strenx® Tube 700MLH 2.0 - 10.00.079 - 0.393 48.3 - 323.91.669 - 12.752 40x40 - 300x3001.575x1.575 - 11.811x11.811 50x30 - 400x2001.969x1.181 - 15.748x7.874 700101 Circular, Square, Rectangular EN 10219-3

                              Strenx® Tube 700MLH

                              Strenx® Tube 700QLH 3.0 - 6.00.118 - 0.236 76.1 - 133.03.000 - 5.236 - - 700101 Circular EN 10210

                              Strenx® Tube 700QLH

                              Strenx® Tube 900MH 4.0 - 6.00.157 - 0.236 139.7 - 244.55.500 - 9.626 100x100 - 200x2003.937x3.937 - 7.874x7.874 120x80 - 250x1504.724x3.149 - 9.843x5.906 900130 Circular, Square, Rectangular EN 10219-3

                              Strenx® Tube 900MH

                              Strenx® Tube 960MH 4.0 - 6.00.157 - 0.236 139.7 - 244.55.500 - 9.626 100x100 - 200x2003.937x3.937 - 7.874x7.874 120x80 - 250x1504.724x3.149 - 9.843x5.906 960139 Circular, Square, Rectangular EN 10219-3

                              Strenx® Tube 960MH

                              Strenx® Tube 960QLH 3.0 - 6.00.118 - 0.236 76.1 - 133.03.000 - 5.236 - - 960140 Circular EN 10210

                              Strenx® Tube 960QLH

                              Compare parameters

                              Select one parameter to compare

                              Comparison

                                Strenx® Sections

                                Strenx® Sections are cold-formed steel section made of hot-rolled, high-strength steel.

                                Hide/Show specific columns Edit
                                Select columns to display
                                  Product Name Thickness range (mminches) Yield strength (min MPaksi) Standards Datasheet
                                  Strenx® Section 650MC 2.5 - 8.00.098 - 0.314 65094 EN 10162
                                  Strenx® Section 700MC 2.5 - 8.00.098 - 0.314 700101 EN 10162
                                  Strenx® Section 900MC 3.0 - 6.00.118 - 0.236 900130 EN 10162
                                  Compare parameters

                                  Select one parameter to compare

                                  Comparison

                                    Strenx® 600

                                    The high-strength structural steel at 600 MPa.

                                    Hide/Show specific columns Edit
                                    Select columns to display
                                      Product Name Thickness range (mminches) Yield strength (min MPaksi) Standards Datasheet
                                      Strenx® 600MC D/E 2.00 - 10.000.079 - 0.393 60087 EN 10149-2

                                      Strenx® 600MC

                                      Compare parameters

                                      Select one parameter to compare

                                      Comparison

                                        Strenx® 650

                                        The high-strength structural steel at 650 MPa.

                                        Hide/Show specific columns Edit
                                        Select columns to display
                                          Product Name Thickness range (mminches) Yield strength (min MPaksi) Standards Datasheet
                                          Strenx® 650MC D/E 2.00 - 10.000.079 - 0.393 65094 EN 10149-2