Strenx performance steel

Strenx® 700MC Plus

Download data sheet

Dimension Range

Strenx® 700MC Plus is available as cut to length sheets in thicknesses of 3.0 - 12.0 mm, widths up to 1525 mm and lengths up to 12300 mm.

Mechanical Properties

Thickness
(mmin)
Thickness
(mmin)
3.0 - 10.00.118 - 0.393
Yield strength ReH 1)
(min MPaksi)
700101
Tensile strength Rm
(MPaksi)
750 - 950109 - 138
Elongation A5
(min %)
13
Min. inner bending radius for a 90° bend 2)
1.0 x t
Thickness
(mmin)
Thickness
(mmin)
10.1 - 12.00.394 - 0.472
Yield strength ReH 1)
(min MPaksi)
700101
Tensile strength Rm
(MPaksi)
750 - 950109 - 138
Elongation A5
(min %)
13
Min. inner bending radius for a 90° bend 2)
1.5 x t

The mechanical properties are tested in the longitudinal direction.

1) If ReH is not applicable then Rp0.2 is used. On thicknesses >8 mm the minimum yield strength may be 20 MPa lower.

2) For both longitudinal and transverse direction.

 

Impact Properties

Product
Product
Strenx® 700MC Plus
Min. impact energy for longitudinal testing,
Charpy V 10x10 mm test specimen 1)
40 J / -60 °C29 ft-lbs / -76 °F

1) Impact testing in the transverse direction is available if specified at the time of the order. Minimum impact energy for transverse testing is 27 J at -40° C.

Impact testing according to EN ISO 148-1 is performed on thicknesses ≥ 5mm. The specified minimum value corresponds to a full-size specimen.

 

Chemical Composition (ladle analysis)

C
(max %)
C
(max %)
0.12
Si
(max %)
0.25
Mn
(max %)
2.10
P
(max %)
0.020
S
(max %)
0.010
Nb
(max %)
0.09 1)
V
(max %)
0.20 1)
Ti
(max %)
0.15 1)

1) Sum of Nb, V and Ti = max 0.22%.

The steel is grain refined.

Carbon Equivalent CET(CEV)

Thickness (mmin)
Thickness (mmin)
Typ CET(CEV)
3.0 - 11.40.118 - 0.452
0.24 (0.38)
11.5 - 12.00.453 - 0.472
0.26 (0.40)

 

Tolerances

More details are given in SSAB’s brochure Strenx® Guarantees.

Thickness

Tolerances according to Strenx® Thickness Guarantee.

Strenx® Guarantees offer considerably narrower thickness tolerances compared to EN 10051. 

Length and Width

Width and length tolerances according to SSAB standard.

SSAB standard offer narrower width and length tolerances compared to EN 10051.

Length tolerances only apply for cut to length sheets.

Shape

Tolerances according to EN 10051. Narrower tolerances according to the SSAB standard are available on request.

Flatness

Tolerances according to Strenx® Flatness Guarantee Class A.

Strenx® Flatness Guarantee offer narrower tolerances compared to EN 10051.

Flatness guarantees only apply for cut to length sheets. 

Surface Properties

According to EN 10163-2 Class A, Subclass 3.

Delivery Conditions

Thermomechanically Rolled. Strenx® 700MC Plus is available in as rolled or pickled surface condition. 

 

Delivery requirements can be found in SSAB’s brochure Strenx® Guarantees or on www.ssab.com.

 

Fabrication and Other Recommendations

Welding, bending and machining

Strenx® 700MC Plus has good welding, cold forming and cutting performance.

 

Strenx® 700MC Plus is a cold forming steel not suited for heat treatments at temperatures above 580°C since the material then maylose its guaranteed properties.

 

For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.

Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.

Strenx® 700MC Plus high-strength structural steel

Strenx® 700MC Plus is a Strenx® grade with exceptional properties for bending and mechanical cutting. It allows you to fast-forward the development of new high-performing load-bearing equipment. It has excellent formability and impact toughness for highly demanding applications, which is particularly important when operating in cold climates. Strenx® 700MC Plus meets or exceeds the requirements of EN 10149-2 grade S700MC. The product has a bendability of Ri/t equal to 1 up to 10 mm (0.393”) thickness. At a thickness above 10 mm (0.393”) the Ri/t value is still as low as 1.5.

Get technical advice

Download our brochure about Strenx® 700MC Plus

Show specs in:

MetricImperial

Ready to upgrade?

Moving up from 700 MPa to 900 MPa means you get almost 30% higher yield strength, which is the case if you upgrade from Strenx® 700MC Plus to Strenx® 900 Plus. Your upgraded equipment has higher load-bearing capacity or can be made with thinner steel for reduced weight. If you are ready to explore the opportunities with a stronger Strenx®, you’re always welcome to get in touch with our steel specialists at SSAB Tech Support or SSAB Knowledge Service Center.

Strenx upgrade icon
Copyright 2026