How to analyze mineral composition and hardness

The mineral composition of abrasives is commonly analyzed using two methods: XRF (X-ray fluorescence) and XRD (X-ray diffraction). The XRF method provides the proportion of oxides, while XRD determines the specific chemical formula of the minerals present.

Granite, a common rock, consists mainly of quartz, alkali feldspar and plagioclase. An XRF analysis of granite would yield oxide proportions such as SiO2, Al2O3 and K2O, while an XRD analysis would identify the mineral composition in detail.

Granite consists of a variety of minerals with different hardnesses.

Mineral
Mineral
 Feldspar
Percentage
 40%
Hardness (HV)
 725
Mineral
Mineral
 Quartz
Percentage
 27%
Hardness (HV)
 1070
Mineral
Mineral
 Biotite
Percentage
 18%
Hardness (HV)
 30-60
Mineral
Mineral
 Plagioclase
Percentage
 15%
Hardness (HV)
725-940

Example of an XRD analysis of granite.

Category and tags

Wear designWear

Contact Technical support


The information in this report is only applicable to SSAB’s products and should not be applied to any other products than original SSAB products. 


This report provides general results and recommendations for SSAB steel products. This report is subject to SSAB’s Terms of Use. It shall be the user's responsibility to verify that the information contained herein is correct and is suitable to be used for the particular purpose and application of the user. The report is intended to be used by professional users only who possess adequate expertise, qualification and knowledge for the safe and correct use of the results and recommendations in this report. This report is provided “as is”. The use of the report is at user’s own discretion and risk and that users will be solely responsible for any use of this report. SSAB disclaims any liability for the content or potential errors of this report, including but not limited to warranties and condition of merchantability or fitness for a particular purpose or suitability for individual applications. SSAB shall not be liable for any kind of direct or indirect damages and/or costs related to or arising therefrom, whether special, incidental, consequential or directly or indirectly related to the use of, or the inability to use, the report or the content, information or results included therein.