SSAB Standard sections

SSAB Standard sections

Standard section steel - cold-formed, dimensionally accurate, strong yet light

SSAB’s cold-formed steel sections are suitable for practically any kind of steel structure, whether for commercial or residential buildings, machines or appliances.

The accuracy of the cross-sectional form and good formability for high-strength material makes it possible to create long-lasting and light structures.

Typical applications are frames and sub-frames, vehicle and trailer bodies, warehouse equipment and masts.

Why choose cold-formed steel sections from SSAB

The benefits of our cold-formed sections include

  • Highly precise shapes in almost any desired length and shape
  • Attractive, smooth surface finish
  • Uniform and consistent product, formed to tight tolerances
  • High strength-to-weight ratio, lightweight product is easy to transport and erect
  • Common jointing methods can be used (welding, bolting, adhesives, etc.)
  • Recyclable at end of life

Explore our open steel section range

Available sections

  • U-section
  • Equal-angles section
  • Unequal-angles section
  • C-section
  • Lipped C-section
  • Conveyor rail
  • Ω-section
  • Z-section
  • Cable cover

See dimensional range below.

Need a custom piece? Visit our tailored sections page. 

Up to standard – for your peace of mind

EN 10162

When you choose cold-formed steel sections from SSAB, you’re investing in materials that meet all the requirements of European standard EN 10162. Our cold-rolled structural steels meet all the technical delivery conditions under this standard, ensuring that you only get the highest quality product.

Introducing C section

SSAB manufactures high-quality C section steel by cold roll forming the steel into a C shape.

The C section consists of a wide web with two parallel flanges on the top and bottom of one side of the web and two lips.

Uses for C section steel

C channel steel often provides structural support in building construction that requires dimensional accuracy and high-quality steel. It is also used in automobiles, ships and other vehicles and to manufacture a variety of industrial, commercial and consumer products.

  • Window and door frames, gates, fences
  • Support for wooden beams
  • Roof rafters
  • Frames in cars, trucks and other vehicles
  • Girts, studs, braces, joists and other structural components
  • Conveyor rails
  • Bridges and truss structures
  • Power transmission towers, solar panel mounts
  • Home appliances, metal furniture

 

C section sizes and grades

We provide C section steel in the standard grade S235J2C+N in a range of sizes. You can request other steel grades, plus custom lengths, punching and more.

Introducing U channel steel

Cold-formed U channel steel is a highly accurate roll formed standard section

SSAB’s cold-formed U channel steel sections are suitable for replacing hot-rolled beams in many applications.

U channel steel sections include a very wide range of options for steel grades as well as steel dimensions. Dimensions exactly matching the application provide significant weight and cost savings. Each unit of weight saved by the U shaped steel channel will offer direct benefits in transportation and in the lighter weight of structures. Our cold-formed U channel steel sections are made according to EN 10162.

Cold-formed U channel steel sections are manufactured by roll forming using SSAB’s high-quality steels. It is mainly used in the construction, transportation and manufacturing industries where dimensional accuracy and high-quality steels are required.

SSAB’s cold-formed steel channels are suitable for replacing hot-rolled beams in many applications.

Replacing hot-rolled UNP beams with cold-formed U channel sections

Hot-rolled UNP beams can often be replaced with cold-formed U channel sections.

 The benefits of using cold-formed U channel steel sections include

  • The accuracy of the cross-sectional form and better straightness compared to the hot-rolled beam.
  • U channel steel dimensions for cold-formed sections are almost unlimited.
  • Cold-formed sections have a wide range of materials and the material can be selected depending on what is most appropriate to the application.
  • Steel U channel sizes can be adjusted to customer needs, thus reducing scrap and the need for further processing.

This U-channel steel series has been developed with the same outside dimensions as hot-rolled UNP beams so that replacing hot-rolled beams is easier. The thickness is selected so that the cold-formed U-channel has the same bending strength, but it weighs less. Weight reduction has been achieved by using higher strength steel grade.

 

Cold-formed U-sections S355MC Hot-rolled UNP-beams S235JR EN 10025-2
h/b t M NR1) VR2) MR3) MR3) VR2) NR1) M UNP
mm/mm mm kg/m kN kN kNm kNm kN kN kg/m
50/38 5 4.27 193 43.8 2.82 2.49 25.4* 167 5.59 50
65/42 5 5.17 234 57.6 4.5 4.16 38.8* 212 7.09 65
80/45 5 6 271 71.2 6.4 6.23 56.4 259 8.64 80
100/50 5 7.17 324 89.3 9.55 9.68 71.1 317 10.6 100
120/55 6 9.91 448 127.6 15.48 14.3 99 400 13.4 120
140/60 6 11.32 512 149.2 20.61 20.3 116 479 16 140
160/65 6 12.73 576 170.7 26.45 27.3 142 564 18.8 160
180/70 7 16.37 740 222.8 37.71
35.3 170 658 22 180
200/75 7 18.02 815 247.8 46.1 44.9 201 757 25.3 200
220/80 8 22.22 1005 309.7 61.59 57.6 234 879 29.4 220
240/85 8 24.1 1090 338.2 72.92 70.5 269 994 33.2 240
260/90 8 25.98 1175 366.7 85.2 87.2 308 1135 37.9 260
280/95 9 31.18 1410 442.8 109.2 105 333 1253 41.8 280
300/100 9 33.3 1506 474.8 125.03 126 358 1382 46.2 300
320/100 11 41.71 1886 610.3 161.29 160 520 1781 59.5 320
350/100 10.5 42.53 1923 635.1 177.71 172 552 1817 60.6 350
400/110 11.5 52.53 2375 792.5 248.54 240 650 2150 71.8 400


Dimensional range

Dimensional range

Availability of stock sections, delivery length 6000 mm for all stock sections excluding cable covers 2500 mm

Dimensions

 

h

(mm)

b

(mm)

 t

(mm)

r

(mm)

M

(kg/m)

16 16 2 2 0.65
20 20 2 2 0.84
25 25 2 2 1.07 
30 30 2 2 1.31 
30 30 3 3 1.89
35 35 2 2 1.54
35 35 3 3

2.24

40 20 2 2 1.15
40 40 2 2 1.78
40 40 3 3 2.59
50(* 20 3 3 1.86
50 25 3 3 2.13
50 30 3 3 2.36
50(* 35 3 3 2.59
50 40 3 3 2.83
50 50 3 3 3.30
50 50 4 4 4.30
60 30 3 3 2.59
60 40 3 3 3.06
70 40 3 3 3.30
70 50 4 4 4.92
80 40 3 3 3.53
80 40 4 4 4.61
80(* 40 5 6 5.60
80 50 4 4 5.24
80 50 5 6 6.39
100(* 30 3 3 3.53
100 50 3 3 4.48
100 50 4 4 5.87
100 50 5 6 7.17
100 50 6 8 8.33
120 40 4 4 5.87
120 50 4 4 6.49
120 60 4 4 7.12
120 60 6 8 10.30
140 60 4 4 7.75
140 60 6 8 11.24
140 70 4 4 8.38
140 70 5 6 10.31
160 60 5 6 10.31
160 60 6 8 12.18
160 70 6 8 13.12
180 70 6 8 14.07
200 60 6 8 14.07
200 70 6 8 15.01
200 80 6 8 16.00
250 75 6 8 17.83

 

Steel grade: S235J2C+N EN 10025-2:2019

*) Available upon request

Dimensions

h

(mm)

 b

(mm)

t

(mm)

r

(mm)

M

(kg/m)

15 15 2 2 0.42
20 20 2 2 0.58
25 25 2 2 0.73
30 30 2 2 0.89
30 30 3 3 1.30
40 40 2 2 1.20
40 40 3 3 1.77
50 50 3 3 2.24
50 50 4 4 2.93
60 60 3 3 2.71
70 70 5 6 5.16
75(* 75 4 4 4.50
80 80 5 6 5.94 

 

Steel grade: S235J2C+N EN 10025-2:2019

*) Available upon request


Dimensions

 

h

(mm)

b

(mm)

t

(mm)

r

(mm)

M

(kg/m)

40 20 2 2 0.89
50 30 3 3 1.77
60 30 3 2 2.00
60 40 3 3 2.24
70 50 4 4 3.56
100 50 4 4 4.50
125 65 5 6 7.12
150 50 5 6 7.51

 

Steel grade: S235J2C+N EN 10025-2:2019


Dimensions

h

(mm)

b

(mm)

a

(mm)

c

(mm)

t

(mm)

r

(mm)

M

(kg/m)

 
28 15 8 12 2 2 0.95 *
30 30 10 10 2 2 1.52  
34 19 8.5 17 2 2 1.19  
50 30 14 22 3 3 2.78  
50 40 10 30 3 3 3.07  
100 50 15 70 3 3 4.95  

 

Steel grade:S235J2C+N EN 10025-2:2019

*) Optional steel grade: DC01 AM EN 10130:2006


Dimensions

h

(mm)

b

(mm)

a

(mm)

e

(mm)

c

(mm)

t

(mm)

r

(mm)

M

(kg/m)

48 26 13 6 22 2 2 1.86
50 30 14 8 22 3 3 2.93

 

Steel grade: S235J2C+N EN 10025-2:2019


Dimensions

h

(mm)

b

(mm)

c

(mm)

d

(mm)

t

(mm)

r

(mm)

M

(kg/m)

 
30 30 8 20 2 2 1.47 *
41 35 10 24 2.5 2.5 2.33   

 

Steel grade: S350GD+Z275MAC EN 10346:2015

*) Optional steel grade: S235J2C+N EN 10025-2:2019


Dimensions

d

(mm)

d outer

(mm)

h

(mm)

t

(mm)

Straight Galvanized SG Bended Galvanized TG
16(* 19 17 1.5(1 x x
25 28 27 1.5(1 x x
35 38 37 1.5(1 x x
45 49 47 2(2 x x
60 64 62 2(2 x -
100 104 102 2(3 x -

 

Delivery length 2500 mm

1) S320GD+Z275MAC EN 10346:2015

2) S350GD+Z275MAC EN 10346:2015

3) S235J2C+N EN 10025-2 (Hot dip galvanized)

*) Shape rectangular


Dimensions

h

(mm)

b

(mm)

a

(mm)

t

(mm)

r

(mm)

M

(kg/m)

53 40 30 3 3 2.66
100 50 50 3 3 4.48
150 50 50 4 4 7.44 

 

Steel grade:S235J2C+N EN 10025-2:2019


Dimensions

 

h

(mm)

b

(mm)

a

(mm)

t

(mm)

r

(mm)

M

(kg/m)

50 35 22 2.5 2.5

3.19

50 60 32 4 8 6.20

 

Steel grade:S235J2C+N EN 10025-2:2019