SSAB Weathering Tube 320WP

Download data sheet

General Product Description

SSAB Weathering Tube 320WP is formable precision tube with anti-corrosive properties, which minimize the need for maintenance and corrosion-prevention treatment.

It is available in circular, rectangular, square and special shapes. Customized shapes and other tailoring options are available upon request. It is typically used in light engineering and construction where corrosion resistance is important. SSAB Weathering Tube 320WP meets or exceeds the standard requirements of EN 10305-3 and COR-TEN A specification.

SSAB Weathering Tubes are manufactured by cold forming and high frequency welding from clean, high quality environmentally friendly steel by modern and efficient tube lines.

Dimension Range

SSAB Weathering Tube 320WP is available in circular, square, rectangular, flat oval and oval (elliptic) shapes.

Shapes
Shapes
Circular (mmin)
Dimensions
16 - 88.90.63 - 3.50
Shapes
Shapes
Square (mmin)
Dimensions
19x19 - 70x70
Shapes
Shapes
Rectangular (mmin)
Dimensions
25x15 - 100x40
Shapes
Shapes
Flat oval (mm)
Dimensions
25x15 - 78x38
Shapes
Shapes
Oval, elliptic (mm)
Dimensions
22x16.5 - 31x17.5
Shapes
Shapes
Wall thickness (mmin)
Dimensions
1.0 - 3.00.039 - 0.12
Shapes
Shapes
Mill length (mm)
Dimensions
6000

Other shapes, sizes and lengths are available upon request.

Circular Dimensions

Outer diameter (mmin)
Outer diameter (mmin)
160.63
1.0 mm (kg/m)
0.370
1.25 mm (kg/m)
—
1.5 mm (kg/m)
—
2.0 mm (kg/m)
—
2.5 mm (kg/m)
—
3.0 mm (kg/m)
—
Outer diameter (mmin)
Outer diameter (mmin)
180.71
1.0 mm (kg/m)
0.419
1.25 mm (kg/m)
—
1.5 mm (kg/m)
—
2.0 mm (kg/m)
—
2.5 mm (kg/m)
—
3.0 mm (kg/m)
—
Outer diameter (mmin)
Outer diameter (mmin)
190.75
1.0 mm (kg/m)
0.444
1.25 mm (kg/m)
0.547
1.5 mm (kg/m)
—
2.0 mm (kg/m)
—
2.5 mm (kg/m)
—
3.0 mm (kg/m)
—
Outer diameter (mmin)
Outer diameter (mmin)
200.79
1.0 mm (kg/m)
0.469
1.25 mm (kg/m)
0.578
1.5 mm (kg/m)
—
2.0 mm (kg/m)
—
2.5 mm (kg/m)
—
3.0 mm (kg/m)
—
Outer diameter (mmin)
Outer diameter (mmin)
220.87
1.0 mm (kg/m)
0.518
1.25 mm (kg/m)
0.640
1.5 mm (kg/m)
—
2.0 mm (kg/m)
—
2.5 mm (kg/m)
—
3.0 mm (kg/m)
—
Outer diameter (mmin)
Outer diameter (mmin)
250.98
1.0 mm (kg/m)
0.592
1.25 mm (kg/m)
0.732
1.5 mm (kg/m)
0.869
2.0 mm (kg/m)
—
2.5 mm (kg/m)
—
3.0 mm (kg/m)
—
Outer diameter (mmin)
Outer diameter (mmin)
281.1
1.0 mm (kg/m)
0.666
1.25 mm (kg/m)
0.825
1.5 mm (kg/m)
0.980
2.0 mm (kg/m)
—
2.5 mm (kg/m)
—
3.0 mm (kg/m)
—
Outer diameter (mmin)
Outer diameter (mmin)
301.2
1.0 mm (kg/m)
0.715
1.25 mm (kg/m)
0.886
1.5 mm (kg/m)
1.05
2.0 mm (kg/m)
1.38
2.5 mm (kg/m)
—
3.0 mm (kg/m)
—
Outer diameter (mmin)
Outer diameter (mmin)
321.3
1.0 mm (kg/m)
0.765
1.25 mm (kg/m)
0.948
1.5 mm (kg/m)
1.13
2.0 mm (kg/m)
1.48
2.5 mm (kg/m)
—
3.0 mm (kg/m)
—
Outer diameter (mmin)
Outer diameter (mmin)
351.4
1.0 mm (kg/m)
0.838
1.25 mm (kg/m)
1.04
1.5 mm (kg/m)
1.24
2.0 mm (kg/m)
1.63
2.5 mm (kg/m)
—
3.0 mm (kg/m)
—
Outer diameter (mmin)
Outer diameter (mmin)
381.5
1.0 mm (kg/m)
0.912
1.25 mm (kg/m)
1.13
1.5 mm (kg/m)
1.35
2.0 mm (kg/m)
1.78
2.5 mm (kg/m)
2.19
3.0 mm (kg/m)
—
Outer diameter (mmin)
Outer diameter (mmin)
401.6
1.0 mm (kg/m)
0.962
1.25 mm (kg/m)
1.20
1.5 mm (kg/m)
1.42
2.0 mm (kg/m)
1.87
2.5 mm (kg/m)
2.31
3.0 mm (kg/m)
—
Outer diameter (mmin)
Outer diameter (mmin)
411.6
1.0 mm (kg/m)
0.990
1.25 mm (kg/m)
1.22
1.5 mm (kg/m)
1.46
2.0 mm (kg/m)
1.92
2.5 mm (kg/m)
2.37
3.0 mm (kg/m)
—
Outer diameter (mmin)
Outer diameter (mmin)
41.51.63
1.0 mm (kg/m)
0.999
1.25 mm (kg/m)
1.24
1.5 mm (kg/m)
1.48
2.0 mm (kg/m)
1.95
2.5 mm (kg/m)
2.40
3.0 mm (kg/m)
—
Outer diameter (mmin)
Outer diameter (mmin)
44.51.75
1.0 mm (kg/m)
1.07
1.25 mm (kg/m)
1.33
1.5 mm (kg/m)
1.59
2.0 mm (kg/m)
2.10
2.5 mm (kg/m)
2.59
3.0 mm (kg/m)
—
Outer diameter (mmin)
Outer diameter (mmin)
481.9
1.0 mm (kg/m)
—
1.25 mm (kg/m)
1.44
1.5 mm (kg/m)
1.72
2.0 mm (kg/m)
2.27
2.5 mm (kg/m)
2.81
3.0 mm (kg/m)
3.33
Outer diameter (mmin)
Outer diameter (mmin)
502.0
1.0 mm (kg/m)
—
1.25 mm (kg/m)
1.50
1.5 mm (kg/m)
1.79
2.0 mm (kg/m)
2.37
2.5 mm (kg/m)
2.93
3.0 mm (kg/m)
3.48
Outer diameter (mmin)
Outer diameter (mmin)
50.82.00
1.0 mm (kg/m)
—
1.25 mm (kg/m)
1.53
1.5 mm (kg/m)
1.82
2.0 mm (kg/m)
2.41
2.5 mm (kg/m)
2.98
3.0 mm (kg/m)
3.54
Outer diameter (mmin)
Outer diameter (mmin)
572.2
1.0 mm (kg/m)
—
1.25 mm (kg/m)
1.72
1.5 mm (kg/m)
2.05
2.0 mm (kg/m)
2.71
2.5 mm (kg/m)
3.36
3.0 mm (kg/m)
4.00
Outer diameter (mmin)
Outer diameter (mmin)
602.4
1.0 mm (kg/m)
—
1.25 mm (kg/m)
1.81
1.5 mm (kg/m)
2.16
2.0 mm (kg/m)
2.86
2.5 mm (kg/m)
3.55
3.0 mm (kg/m)
4.22
Outer diameter (mmin)
Outer diameter (mmin)
702.8
1.0 mm (kg/m)
—
1.25 mm (kg/m)
—
1.5 mm (kg/m)
2.53
2.0 mm (kg/m)
3.35
2.5 mm (kg/m)
4.16
3.0 mm (kg/m)
4.96
Outer diameter (mmin)
Outer diameter (mmin)
76.13.00
1.0 mm (kg/m)
—
1.25 mm (kg/m)
—
1.5 mm (kg/m)
2.76
2.0 mm (kg/m)
3.65
2.5 mm (kg/m)
4.54
3.0 mm (kg/m)
5.41
Outer diameter (mmin)
Outer diameter (mmin)
88.93.50
1.0 mm (kg/m)
—
1.25 mm (kg/m)
—
1.5 mm (kg/m)
—
2.0 mm (kg/m)
4.29
2.5 mm (kg/m)
5.33
3.0 mm (kg/m)
6.36

Square Dimensions

Height x Width (mm)
Height x Width (mm)
19 x 19
1.0 mm (kg/m)
0.564
1.25 mm (kg/m)
0.694
1.5 mm (kg/m)
0.820
2.0 mm (kg/m)
—
2.5 mm (kg/m)
—
3.0 mm (kg/m)
—
Height x Width (mm)
Height x Width (mm)
20 x 20
1.0 mm (kg/m)
0.595
1.25 mm (kg/m)
0.733
1.5 mm (kg/m)
0.868
2.0 mm (kg/m)
—
2.5 mm (kg/m)
—
3.0 mm (kg/m)
—
Height x Width (mm)
Height x Width (mm)
25 x 25
1.0 mm (kg/m)
0.752
1.25 mm (kg/m)
0.930
1.5 mm (kg/m)
1.10
2.0 mm (kg/m)
1.44
2.5 mm (kg/m)
—
3.0 mm (kg/m)
—
Height x Width (mm)
Height x Width (mm)
30 x 30
1.0 mm (kg/m)
0.909
1.25 mm (kg/m)
1.13
1.5 mm (kg/m)
1.34
2.0 mm (kg/m)
1.75
2.5 mm (kg/m)
2.15
3.0 mm (kg/m)
—
Height x Width (mm)
Height x Width (mm)
32 x 32
1.0 mm (kg/m)
0.972
1.25 mm (kg/m)
1.20
1.5 mm (kg/m)
1.43
2.0 mm (kg/m)
1.88
2.5 mm (kg/m)
2.31
3.0 mm (kg/m)
—
Height x Width (mm)
Height x Width (mm)
35 x 35
1.0 mm (kg/m)
1.07
1.25 mm (kg/m)
1.32
1.5 mm (kg/m)
1.57
2.0 mm (kg/m)
2.07
2.5 mm (kg/m)
2.54
3.0 mm (kg/m)
—
Height x Width (mm)
Height x Width (mm)
40 x 40
1.0 mm (kg/m)
—
1.25 mm (kg/m)
1.52
1.5 mm (kg/m)
1.81
2.0 mm (kg/m)
2.38
2.5 mm (kg/m)
2.93
3.0 mm (kg/m)
3.33
Height x Width (mm)
Height x Width (mm)
50 x 50
1.0 mm (kg/m)
—
1.25 mm (kg/m)
1.91
1.5 mm (kg/m)
2.28
2.0 mm (kg/m)
3.01
2.5 mm (kg/m)
3.72
3.0 mm (kg/m)
4.28
Height x Width (mm)
Height x Width (mm)
60 x 60
1.0 mm (kg/m)
—
1.25 mm (kg/m)
—
1.5 mm (kg/m)
2.75
2.0 mm (kg/m)
3.64
2.5 mm (kg/m)
4.50
3.0 mm (kg/m)
5.22
Height x Width (mm)
Height x Width (mm)
70 x 70
1.0 mm (kg/m)
—
1.25 mm (kg/m)
—
1.5 mm (kg/m)
—
2.0 mm (kg/m)
4.26
2.5 mm (kg/m)
5.29
3.0 mm (kg/m)
6.16

Rectangular Dimensions

Height x Width (mm)
Height x Width (mm)
25 x 15
1.0 mm (kg/m)
0.595
1.25 mm (kg/m)
0.733
1.5 mm (kg/m)
0.868
2.0 mm (kg/m)
—
2.5 mm (kg/m)
—
3.0 mm (kg/m)
—
Height x Width (mm)
Height x Width (mm)
30 x 10
1.0 mm (kg/m)
0.595
1.25 mm (kg/m)
0.733
1.5 mm (kg/m)
0.868
2.0 mm (kg/m)
—
2.5 mm (kg/m)
—
3.0 mm (kg/m)
—
Height x Width (mm)
Height x Width (mm)
30 x 15
1.0 mm (kg/m)
0.673
1.25 mm (kg/m)
0.831
1.5 mm (kg/m)
0.985
2.0 mm (kg/m)
—
2.5 mm (kg/m)
—
3.0 mm (kg/m)
—
Height x Width (mm)
Height x Width (mm)
30 x 20
1.0 mm (kg/m)
0.752
1.25 mm (kg/m)
0.930
1.5 mm (kg/m)
1.10
2.0 mm (kg/m)
1.44
2.5 mm (kg/m)
—
3.0 mm (kg/m)
—
Height x Width (mm)
Height x Width (mm)
30 x 25
1.0 mm (kg/m)
0.830
1.25 mm (kg/m)
1.03
1.5 mm (kg/m)
1.22
2.0 mm (kg/m)
1.59
2.5 mm (kg/m)
—
3.0 mm (kg/m)
—
Height x Width (mm)
Height x Width (mm)
35 x 15
1.0 mm (kg/m)
0.752
1.25 mm (kg/m)
0.930
1.5 mm (kg/m)
1.10
2.0 mm (kg/m)
1.44
2.5 mm (kg/m)
—
3.0 mm (kg/m)
—
Height x Width (mm)
Height x Width (mm)
35 x 20
1.0 mm (kg/m)
0.830
1.25 mm (kg/m)
1.03
1.5 mm (kg/m)
1.22
2.0 mm (kg/m)
1.59
2.5 mm (kg/m)
—
3.0 mm (kg/m)
—
Height x Width (mm)
Height x Width (mm)
40 x 20
1.0 mm (kg/m)
0.909
1.25 mm (kg/m)
1.13
1.5 mm (kg/m)
1.34
2.0 mm (kg/m)
1.75
2.5 mm (kg/m)
2.15
3.0 mm (kg/m)
—
Height x Width (mm)
Height x Width (mm)
40 x 25
1.0 mm (kg/m)
0.987
1.25 mm (kg/m)
1.22
1.5 mm (kg/m)
1.46
2.0 mm (kg/m)
1.91
2.5 mm (kg/m)
2.34
3.0 mm (kg/m)
—
Height x Width (mm)
Height x Width (mm)
40 x 30
1.0 mm (kg/m)
1.07
1.25 mm (kg/m)
1.32
1.5 mm (kg/m)
1.57
2.0 mm (kg/m)
2.07
2.5 mm (kg/m)
2.54
3.0 mm (kg/m)
—
Height x Width (mm)
Height x Width (mm)
50 x 20
1.0 mm (kg/m)
1.07
1.25 mm (kg/m)
1.32
1.5 mm (kg/m)
1.57
2.0 mm (kg/m)
2.07
2.5 mm (kg/m)
2.54
3.0 mm (kg/m)
—
Height x Width (mm)
Height x Width (mm)
50 x 25
1.0 mm (kg/m)
—
1.25 mm (kg/m)
1.42
1.5 mm (kg/m)
1.69
2.0 mm (kg/m)
2.22
2.5 mm (kg/m)
2.74
3.0 mm (kg/m)
3.10
Height x Width (mm)
Height x Width (mm)
50 x 30
1.0 mm (kg/m)
—
1.25 mm (kg/m)
1.52
1.5 mm (kg/m)
1.81
2.0 mm (kg/m)
2.38
2.5 mm (kg/m)
2.93
3.0 mm (kg/m)
3.33
Height x Width (mm)
Height x Width (mm)
50 x 40
1.0 mm (kg/m)
—
1.25 mm (kg/m)
1.71
1.5 mm (kg/m)
2.05
2.0 mm (kg/m)
2.69
2.5 mm (kg/m)
3.33
3.0 mm (kg/m)
3.80
Height x Width (mm)
Height x Width (mm)
60 x 20
1.0 mm (kg/m)
—
1.25 mm (kg/m)
1.52
1.5 mm (kg/m)
1.81
2.0 mm (kg/m)
2.38
2.5 mm (kg/m)
2.93
3.0 mm (kg/m)
3.33
Height x Width (mm)
Height x Width (mm)
60 x 30
1.0 mm (kg/m)
—
1.25 mm (kg/m)
1.71
1.5 mm (kg/m)
2.05
2.0 mm (kg/m)
2.69
2.5 mm (kg/m)
3.33
3.0 mm (kg/m)
3.80
Height x Width (mm)
Height x Width (mm)
60 x 40
1.0 mm (kg/m)
—
1.25 mm (kg/m)
1.91
1.5 mm (kg/m)
2.28
2.0 mm (kg/m)
3.01
2.5 mm (kg/m)
3.72
3.0 mm (kg/m)
4.28
Height x Width (mm)
Height x Width (mm)
70 x 25
1.0 mm (kg/m)
—
1.25 mm (kg/m)
—
1.5 mm (kg/m)
2.16
2.0 mm (kg/m)
2.85
2.5 mm (kg/m)
3.52
3.0 mm (kg/m)
4.04
Height x Width (mm)
Height x Width (mm)
70 x 30
1.0 mm (kg/m)
—
1.25 mm (kg/m)
—
1.5 mm (kg/m)
2.28
2.0 mm (kg/m)
3.01
2.5 mm (kg/m)
3.72
3.0 mm (kg/m)
4.28
Height x Width (mm)
Height x Width (mm)
70 x 50
1.0 mm (kg/m)
—
1.25 mm (kg/m)
—
1.5 mm (kg/m)
2.75
2.0 mm (kg/m)
3.64
2.5 mm (kg/m)
4.50
3.0 mm (kg/m)
5.22
Height x Width (mm)
Height x Width (mm)
80 x 20
1.0 mm (kg/m)
—
1.25 mm (kg/m)
—
1.5 mm (kg/m)
2.28
2.0 mm (kg/m)
3.01
2.5 mm (kg/m)
3.72
3.0 mm (kg/m)
4.28
Height x Width (mm)
Height x Width (mm)
80 x 30
1.0 mm (kg/m)
—
1.25 mm (kg/m)
—
1.5 mm (kg/m)
2.52
2.0 mm (kg/m)
3.32
2.5 mm (kg/m)
4.11
3.0 mm (kg/m)
4.74
Height x Width (mm)
Height x Width (mm)
80 x 40
1.0 mm (kg/m)
—
1.25 mm (kg/m)
—
1.5 mm (kg/m)
2.75
2.0 mm (kg/m)
3.64
2.5 mm (kg/m)
4.50
3.0 mm (kg/m)
5.22
Height x Width (mm)
Height x Width (mm)
80 x 60
1.0 mm (kg/m)
—
1.25 mm (kg/m)
—
1.5 mm (kg/m)
—
2.0 mm (kg/m)
4.26
2.5 mm (kg/m)
5.29
3.0 mm (kg/m)
6.16
Height x Width (mm)
Height x Width (mm)
100 x 40
1.0 mm (kg/m)
—
1.25 mm (kg/m)
—
1.5 mm (kg/m)
—
2.0 mm (kg/m)
4.26
2.5 mm (kg/m)
5.29
3.0 mm (kg/m)
6.16

Flat Oval Dimensions

Height x Width (mm)
Height x Width (mm)
25 x 15
1.0 mm (kg/m)
0.502
1.25 mm (kg/m)
0.620
1.5 mm (kg/m)
0.735
2.0 mm (kg/m)
—
2.5 mm (kg/m)
—
Height x Width (mm)
Height x Width (mm)
30 x 15
1.0 mm (kg/m)
0.581
1.25 mm (kg/m)
0.718
1.5 mm (kg/m)
0.853
2.0 mm (kg/m)
—
2.5 mm (kg/m)
—
Height x Width (mm)
Height x Width (mm)
35 x 15
1.0 mm (kg/m)
0.659
1.25 mm (kg/m)
0.816
1.5 mm (kg/m)
0.970
2.0 mm (kg/m)
1.269
2.5 mm (kg/m)
—
Height x Width (mm)
Height x Width (mm)
40 x 20
1.0 mm (kg/m)
0.783
1.25 mm (kg/m)
0.971
1.5 mm (kg/m)
1.155
2.0 mm (kg/m)
1.516
2.5 mm (kg/m)
—
Height x Width (mm)
Height x Width (mm)
40 x 25
1.0 mm (kg/m)
0.827
1.25 mm (kg/m)
1.03
1.5 mm (kg/m)
1.22
2.0 mm (kg/m)
1.61
2.5 mm (kg/m)
—
Height x Width (mm)
Height x Width (mm)
45 x 25
1.0 mm (kg/m)
0.906
1.25 mm (kg/m)
1.125
1.5 mm (kg/m)
1.340
2.0 mm (kg/m)
1.762
2.5 mm (kg/m)
—
Height x Width (mm)
Height x Width (mm)
50 x 20
1.0 mm (kg/m)
0.940
1.25 mm (kg/m)
1.167
1.5 mm (kg/m)
1.391
2.0 mm (kg/m)
1.830
2.5 mm (kg/m)
—
Height x Width (mm)
Height x Width (mm)
60 x 15
1.0 mm (kg/m)
1.052
1.25 mm (kg/m)
1.307
1.5 mm (kg/m)
1.559
2.0 mm (kg/m)
2.054
2.5 mm (kg/m)
—
Height x Width (mm)
Height x Width (mm)
78 x 38
1.0 mm (kg/m)
—
1.25 mm (kg/m)
1.918
1.5 mm (kg/m)
2.292
2.0 mm (kg/m)
3.032
2.5 mm (kg/m)
3.759

Oval Dimensions

Height x Width (mm)
Height x Width (mm)
22 x 16.5
1.0 mm (kg/m)
0.450
1.25 mm (kg/m)
0.555
1.5 mm (kg/m)
—
Height x Width (mm)
Height x Width (mm)
31 x 17.5
1.0 mm (kg/m)
0.573
1.25 mm (kg/m)
0.709
1.5 mm (kg/m)
0.842

Mechanical Properties

Yield strength Rp0.2
(min MPa)
Yield strength Rp0.2
(min MPa)
320
Tensile strength Rm
(min MPa)
410
Elongation A
(min %)
19

Mechanical properties meet the requirements of EN 10305 (+CR2).

Chemical Composition (ladle analysis)

C
(max %)
C
(max %)
0.12
Si
(max %)
0.75
Mn
(max %)
0.50
P
(max %)
0.15
S
(max %)
0.03
Altot
(min %)
0.01

Tolerances

Tolerance Circular

Characteristic
Characteristic
Outside diameter (D) (1
D < 20 mm
20 ≤ D < 32 mm
32 ≤ D < 44 mm
44 ≤ D < 55 mm
55 ≤ D < 70 mm
70 ≤ D < 80 mm
80 ≤ D < 100 mm
Circular precision tubes
Tolerances meet or exceed the requirements of EN 10305-3

±0.12 mm
±0.15 mm
±0.20 mm
±0.25 mm
±0.30 mm
±0.35 mm
±0.40 mm
Characteristic
Characteristic
Out-of-roundness
Circular precision tubes
Tolerances meet or exceed the requirements of EN 10305-3
The diameter tolerances include the out-of-roundness
Characteristic
Characteristic
Thickness (T)
Circular precision tubes
Tolerances meet or exceed the requirements of EN 10305-3
T ≤ 1.5 mm: ±0.15 mm
T>1.5 mm: ±10% of nominal thickness or ±0.35 mm whichever is the smaller
Characteristic
Characteristic
Straightness
Circular precision tubes
Tolerances meet or exceed the requirements of EN 10305-3
Maximum 0.15% of measured length
Characteristic
Characteristic
Height of internal weld bead, g;
Bead removed
Bead not removed
Circular precision tubes
Tolerances meet or exceed the requirements of EN 10305-3

g ≤ 0.3 mm
g < 0.6 mm, when T ≤ 1.5 mm
g < 0.4 x T, when 1.5 mm < T ≤ 3.0 mm
Characteristic
Characteristic
Mill length
Circular precision tubes
Tolerances meet or exceed the requirements of EN 10305-3
0/+50 mm, standard length 6000 mm
Characteristic
Characteristic
Exact length, single cutting
Circular precision tubes
Tolerances meet or exceed the requirements of EN 10305-3
Agreed at the time of enquiry and order
Characteristic
Characteristic
Exact length, bundle cutting
Circular precision tubes
Tolerances meet or exceed the requirements of EN 10305-3
Agreed at the time of enquiry and order

1)For a maximum distance of 100 mm, the ends may, due to the cutting method, have diameters outside the tolerances.

Tolerance Square

Characteristic
Characteristic
Outside dimensions (H) and (B), longer side1)
H < 25 mm
25 ≤ H < 40 mm
40 ≤ H < 60 mm
60≤ H < 70 mm
70 ≤ H < 80 mm
Square precision tubes
Tolerances meet or exceed the requirements of EN 10305-3

±0.20 mm
±0.25 mm
±0.30 mm
±0.35 mm
±0.40 mm
Characteristic
Characteristic
Side concavity and convexity
Square precision tubes
Tolerances meet or exceed the requirements of EN 10305-3
Included in outside dimension tolerance
Characteristic
Characteristic
Thickness (T)
Square precision tubes
Tolerances meet or exceed the requirements of EN 10305-3
T ≤ 1.5 mm: ±0.15 mm
T>1.5 mm: ±10% of nominal thickness or ±0.35 mm whichever is the smaller
Characteristic
Characteristic
Straightness
Square precision tubes
Tolerances meet or exceed the requirements of EN 10305-3
Maximum 0.15% of measured tube length when shorter side length > 30 mm
Maximum 0.25% of measured tube length when the shorter side length ≤ 30 mm
Characteristic
Characteristic
Location of weld seam from the centre line
Square precision tubes
Tolerances meet or exceed the requirements of EN 10305-3
On narrow side for square and rectangular, optionally on wide side. On wide side for flat oval and ellipse. ± 10% of side length or ± 3 mm, whichever is greater.
Characteristic
Characteristic
Height of internal weld bead, g;
Bead removed
Bead not removed
Square precision tubes
Tolerances meet or exceed the requirements of EN 10305-3

g ≤ 0.3 mm
g < 0.6 mm, when T ≤ 1.5 mm
g < 0.4 x T, when 1.5 mm < T ≤ 3.0 mm
Characteristic
Characteristic
Squareness of side
Square precision tubes
Tolerances meet or exceed the requirements of EN 10305-3
90° ±1°
Characteristic
Characteristic
Corner profile
Square precision tubes
Tolerances meet or exceed the requirements of EN 10305-3
R < 1.5 x T, when T ≤ 2.5 mm
R < 2.2 x T, when T > 2.5 mm
Characteristic
Characteristic
Twist (V)
Square precision tubes
Tolerances meet or exceed the requirements of EN 10305-3
V ≤ 3 mm for B and H ≤ 30 mm
V ≤ B/10 or ≤ H/10 for B or H > 30 mm
Characteristic
Characteristic
Mill length
Square precision tubes
Tolerances meet or exceed the requirements of EN 10305-3
0/+50 mm, standard length 6000 mm
Characteristic
Characteristic
Exact length, single cutting
Square precision tubes
Tolerances meet or exceed the requirements of EN 10305-3
Agreed at the time of enquiry and order
Characteristic
Characteristic
Exact length, bundle cutting
Square precision tubes
Tolerances meet or exceed the requirements of EN 10305-3
Agreed at the time of enquiry and order

1)For a maximum distance of 100 mm, the ends may, due to the cutting method, have diameters outside the tolerances.

Tolerance Rectangular

Characteristic
Characteristic
Outside dimensions (H) and (B), longer side1)
H < 25 mm
25 ≤ H < 40 mm
40 ≤ H < 60 mm
60≤ H < 70 mm
70 ≤ H < 80 mm
80 ≤ H < 90 mm
90 ≤ H < 100 mm
100 ≤ H < 120 mm
Rectangular precision tubes
Tolerances meet or exceed the requirements of EN 10305-3

±0.20 mm
±0.25 mm
±0.30 mm
±0.35 mm
±0.40 mm
±0.50 mm
±0.60 mm
±0.65 mm
Characteristic
Characteristic
Side concavity and convexity
Rectangular precision tubes
Tolerances meet or exceed the requirements of EN 10305-3
Included in outside dimension tolerance
Characteristic
Characteristic
Thickness (T)
Rectangular precision tubes
Tolerances meet or exceed the requirements of EN 10305-3
T ≤ 1.5 mm: ±0.15 mm
T>1.5 mm: ±10% of nominal thickness or ±0.35 mm whichever is the smaller
Characteristic
Characteristic
Straightness
Rectangular precision tubes
Tolerances meet or exceed the requirements of EN 10305-3
Maximum 0.15% of measured tube length when shorter side length > 30 mm
Maximum 0.25% of measured tube length when the shorter side length ≤ 30 mm
Characteristic
Characteristic
Location of weld seam from the centre line
Rectangular precision tubes
Tolerances meet or exceed the requirements of EN 10305-3
On narrow side for square and rectangular, optionally on wide side. On wide side for flat oval and ellipse. ± 10% of side length or ± 3 mm, whichever is greater.
Characteristic
Characteristic
Height of internal weld bead, g;
Bead removed
Bead not removed
Rectangular precision tubes
Tolerances meet or exceed the requirements of EN 10305-3

g ≤ 0.3 mm
g < 0.6 mm, when T ≤ 1.5 mm
g < 0.4 x T, when 1.5 mm < T ≤ 3.0 mm
Characteristic
Characteristic
Squareness of side
Rectangular precision tubes
Tolerances meet or exceed the requirements of EN 10305-3
90° ±1°
Characteristic
Characteristic
Corner profile
Rectangular precision tubes
Tolerances meet or exceed the requirements of EN 10305-3
R < 1.5 x T, when T ≤ 2.5 mm
R < 2.2 x T, when T > 2.5 mm
Characteristic
Characteristic
Twist (V)
Rectangular precision tubes
Tolerances meet or exceed the requirements of EN 10305-3
V ≤ 3 mm for B and H ≤ 30 mm
V ≤ B/10 or ≤ H/10 for B or H > 30 mm
Characteristic
Characteristic
Mill length
Rectangular precision tubes
Tolerances meet or exceed the requirements of EN 10305-3
0/+50 mm, standard length 6000 mm
Characteristic
Characteristic
Exact length, single cutting
Rectangular precision tubes
Tolerances meet or exceed the requirements of EN 10305-3
Agreed at the time of enquiry and order
Characteristic
Characteristic
Exact length, bundle cutting
Rectangular precision tubes
Tolerances meet or exceed the requirements of EN 10305-3
Agreed at the time of enquiry and order

1)For a maximum distance of 100 mm, the ends may, due to the cutting method, have diameters outside the tolerances.

Tolerance Flat Oval

Characteristic
Characteristic
Outside dimensions (H) and (B), longer side1)
H < 25 mm
25 ≤ H < 40 mm
40 ≤ H < 60 mm
60≤ H < 70 mm
70 ≤ H < 80 mm
80 ≤ H < 90 mm
90 ≤ H < 100 mm
100 ≤ H < 120 mm
Flat oval precision tubes
Tolerances meet or exceed the requirements of EN 10305-3

±0.20 mm
±0.25 mm
±0.30 mm
±0.35 mm
±0.40 mm
Characteristic
Characteristic
Concavity/convexity
Flat oval precision tubes
Tolerances meet or exceed the requirements of EN 10305-3
Included in outside dimension tolerance
Characteristic
Characteristic
Thickness (T)
Flat oval precision tubes
Tolerances meet or exceed the requirements of EN 10305-3
T ≤ 1.5 mm: ±0.15 mm
T>1.5 mm: ±10% of nominal thickness or ±0.35 mm whichever is the smaller
Characteristic
Characteristic
Straightness
Flat oval precision tubes
Tolerances meet or exceed the requirements of EN 10305-3
Maximum 0.15% of measured tube length when shorter side length > 30 mm
Maximum 0.25% of measured tube length when the shorter side length ≤ 30 mm
Characteristic
Characteristic
Location of weld seam from the centre line
Flat oval precision tubes
Tolerances meet or exceed the requirements of EN 10305-3
On narrow side for square and rectangular, optionally on wide side. On wide side for flat oval and ellipse. ± 10% of side length or ± 3 mm, whichever is greater.
Characteristic
Characteristic
Height of internal weld bead, g;
Bead removed
Bead not removed
Flat oval precision tubes
Tolerances meet or exceed the requirements of EN 10305-3

g ≤ 0.3 mm
g < 0.6 mm, when T ≤ 1.5 mm
g < 0.4 x T, when 1.5 mm < T ≤ 3.0 mm
Characteristic
Characteristic
Mill length
Flat oval precision tubes
Tolerances meet or exceed the requirements of EN 10305-3
0/+50 mm, standard length 6000 mm
Characteristic
Characteristic
Exact length, single cutting
Flat oval precision tubes
Tolerances meet or exceed the requirements of EN 10305-3
Agreed at the time of enquiry and order
Characteristic
Characteristic
Exact length, bundle cutting
Flat oval precision tubes
Tolerances meet or exceed the requirements of EN 10305-3
Agreed at the time of enquiry and order

1)For a maximum distance of 100 mm, the ends may, due to the cutting method, have diameters outside the tolerances.

Tolerance Oval

Characteristic
Characteristic
Outside dimensions (H) and (B), longer side1)
H < 25 mm
25 ≤ H < 40 mm
40 ≤ H < 60 mm
60≤ H < 70 mm
70 ≤ H < 80 mm
80 ≤ H < 90 mm
90 ≤ H < 100 mm
100 ≤ H < 120 mm
Oval (elliptic) precision tubes
Tolerances meet or exceed the requirements of EN 10305-3

±0.20 mm
±0.25 mm
Characteristic
Characteristic
Concavity/convexity
Oval (elliptic) precision tubes
Tolerances meet or exceed the requirements of EN 10305-3
Included in outside dimension tolerance
Characteristic
Characteristic
Thickness (T)
Oval (elliptic) precision tubes
Tolerances meet or exceed the requirements of EN 10305-3
T ≤ 1.5 mm: ±0.15 mm
T>1.5 mm: ±10% of nominal thickness or ±0.35 mm whichever is the smaller
Characteristic
Characteristic
Straightness
Oval (elliptic) precision tubes
Tolerances meet or exceed the requirements of EN 10305-3
Maximum 0.15% of measured tube length when shorter side length > 30 mm
Maximum 0.25% of measured tube length when the shorter side length ≤ 30 mm
Characteristic
Characteristic
Location of weld seam from the centre line
Oval (elliptic) precision tubes
Tolerances meet or exceed the requirements of EN 10305-3
On narrow side for square and rectangular, optionally on wide side. On wide side for flat oval and ellipse. ± 10% of side length or ± 3 mm, whichever is greater.
Characteristic
Characteristic
Height of internal weld bead, g;
Bead removed
Bead not removed
Oval (elliptic) precision tubes
Tolerances meet or exceed the requirements of EN 10305-3

g ≤ 0.3 mm
g < 0.6 mm, when T ≤ 1.5 mm
g < 0.4 x T, when 1.5 mm < T ≤ 3.0 mm
Characteristic
Characteristic
Mill length
Oval (elliptic) precision tubes
Tolerances meet or exceed the requirements of EN 10305-3
0/+50 mm, standard length 6000 mm
Characteristic
Characteristic
Exact length, single cutting
Oval (elliptic) precision tubes
Tolerances meet or exceed the requirements of EN 10305-3
Agreed at the time of enquiry and order
Characteristic
Characteristic
Exact length, bundle cutting
Oval (elliptic) precision tubes
Tolerances meet or exceed the requirements of EN 10305-3
Agreed at the time of enquiry and order

1)For a maximum distance of 100 mm, the ends may, due to the cutting method, have diameters outside the tolerances.