SSAB Laser® 355ML Plus

Download data sheet

General Product Description

SSAB Laser® 355ML Plus is an advanced thermomechanically rolled weldable fine grain steel for laser cutting and cold forming. The SSAB guarantee for flatness, both before and after laser cutting, is ≤ 3 mm/m deviation.

SSAB Laser® 355ML Plus meets and exceeds the requirements of S355ML in EN 10025-4. Dual certification and CE marking are available upon request.

Dimension Range

SSAB Laser® 355ML Plus

Delivery form
Hot rolled plate
Thickness
(mmin)
8.0 - 30.00.31 - 1.18
Width
(mmin)
1000 - 330039.37 - 129.9
Length
(mmin)
2000 - 1500078.74 - 590.55

Mechanical Properties

Yield strength ReH
(min MPa)
Yield strength ReH
(min MPa)
355
Tensile strength Rm
(MPa)
470 - 630
Elongation A5
(min %)
22
Min. inner bending radius for a 90° bend 1)
(x t)
1.0

The mechanical properties are tested transverse to the direction of rolling.

1) The bending guarantee is valid for both longitudinal and transverse direction.

Impact Properties

Min. impact energy for longitudinal testing,
Charpy V 10x10 mm test specimens
Min. impact energy for longitudinal testing,
Charpy V 10x10 mm test specimens
40 J / -50 °C
Impact testing according to EN ISO 148-1 is performed on thicknesses ≥ 6mm. The specified minimum value corresponds to a full-size specimen.

Chemical Composition (heat analysis)

C
(max %)
C
(max %)
0.12
Si
(max %)
0.03
Mn
(max %)
1.60
P
(max %)
0.020
S
(max %)
0.015
CEV
(max )
0.38

All SSAB Laser® steels are aluminum-killed (Al ≥ 0.015%) and grain-refined. Additionally, niobium (Nb), vanadium (V), titanium (Ti) and/or boron (B) may be used as single alloying element or in any combination.

Tolerances

All SSAB Laser® products are delivered with SSAB Laser® tolerances, which means increased guarantees compared to corresponding EN standards. Detailed information is available on ssab.com.

Thickness

SSAB Laser® tolerances correspond to 3/4 of EN 10029 as default.

Width

-0/+4-10mm depending on the thickness.

Length

Nominal length
(mm)
Nominal length
(mm)
2000 ˂ l ≤ 10000
Tolerance
(mm)
- 0 / + 15
Nominal length
(mm)
Nominal length
(mm)
10000 ˂ l ≤ 15000
Tolerance
(mm)
- 0 / + 20

Shape

Tolerances according to EN 10029.

Flatness

≤ 3 mm/m flatness deviation for both delivery condition and laser cut parts.

Surface Properties

According to EN 10163-2 Class A, Subclass 3.

Delivery Conditions

Thermomechanically rolled.

Surface and edge condition

Hot rolled plate: as rolled surface condition and cut edges as default.

Fabrication and Other Recommendations

All SSAB Laser® products have been optimized for laser cutting, cold forming and welding.

SSAB Laser® ML Plus products are thermomechanically rolled weldable fine grain steels for laser cutting and cold forming. It is not suited for heat treatments at temperatures above 580°C, since the material then may lose its guaranteed properties.

For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.

Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.

Contact Information

www.ssab.com/contact 
Copyright 2026