SSAB Boron 45

Download data sheet

Compared to conventional B27/B30 steel, SSAB Boron 45 delivers 4 to 5 HRC higher hardness that goes all the way through its thickness. It can be used with a variety of common heat treatment processes, including press hardening and hot forming – without quench cracks.

SSAB Boron 45’s excellent batch-to-batch consistency helps you make disc harrows and cultivators with a highly dependable through-thickness hardness for longer service life. Plus, SSAB Boron 45 has good toughness to absorb the impact from stones and small rocks.

SSAB Boron 45 is easy to cut and machine. If you need to punch or cold form SSAB Boron 45, order the hot-rolled annealed condition.

Hardness of SSAB Boron 45 compared to B27/B30

Hardness of SSAB Boron 45 compared to B27/B30

Typical surface hardness (HRC), not guaranteed, measured at 1,5 mm from surface.

General Product Description

SSAB Boron 45 is steel for quench- and press hardening. The degree of hardness and toughness that can be achieved after heat-treatment will provide the final products with wear- and shock resistance properties that assure longer lifetime.

Dimension Range

SSAB Boron 45 is available in thickness range 3.00-10.00 mm and widths up to 1800 mm as coils, slit coils and cut-to-length sheets. Lengths up to 13 meters as cut to length.

Mechanical Properties

Condition
Condition
Hot rolled
Typical yield strength
(MPa), not guaranteed
440
Typical tensile strength
(MPa), not guaranteed
660
Typical Elongation A (%),
not guaranteed
18
Typical Hardness
(HRC), not guaranteed
—
Typical hardness
(HBW), not guaranteed
190
Condition
Condition
Hot rolled annealed
Typical yield strength
(MPa), not guaranteed
370
Typical tensile strength
(MPa), not guaranteed
570
Typical Elongation A (%),
not guaranteed
24
Typical Hardness
(HRC), not guaranteed
—
Typical hardness
(HBW), not guaranteed
175
Condition
Condition
Hot rolled water quenched
Typical yield strength
(MPa), not guaranteed
—
Typical tensile strength
(MPa), not guaranteed
—
Typical Elongation A (%),
not guaranteed
—
Typical Hardness
(HRC), not guaranteed
60
Typical hardness
(HBW), not guaranteed
—
Condition
Condition
Hot rolled oil quenched
Typical yield strength
(MPa), not guaranteed
—
Typical tensile strength
(MPa), not guaranteed
—
Typical Elongation A (%),
not guaranteed
—
Typical Hardness
(HRC), not guaranteed
57
Typical hardness
(HBW), not guaranteed
596

Bending radius

For further information, please consult your local SSAB contact person or contact SSAB's Technical Customer Service.

Material Testing

A test certificate according to EN 10204/3.1 (chemical composition only) is part of the delivery.

A test certificate according to EN 10204/3.1 (with mechanical test) can be provided by special agreement only.

Chemical Composition (heat analysis)

Condition
Condition
Hot rolled strip
C
(%)
0.42 - 0.47
Si
(%)
0.10 - 0.30
Mn
(%)
0.70 - 1.00
S
(max %)
0.010
P
(max %)
0.020
Cr
(%)
0.30 - 0.80
B
(%)
0.0008 - 0.0050

The steel is grain refined.

Carbon Equivalent CEV

Condition
Condition
Typical CEV (%)
Hot rolled strip
0.71

Tolerances

SSAB Boron steels are delivered with SSAB Boron tolerances which meet and exceed the requirements in corresponding EN standards. Tighter tolerances are available on request.

Thickness

Hot rolled coils and sheet products: according to SSAB Boron thickness tolerances that exceed EN 10051 and correspond to 2/3 of EN 10051 as default value.

Length and Width

Hot rolled coils and sheets with mill edges: SSAB Boron width tolerances are corresponding to -0/+20 mm.

Hot rolled coils and sheets with cut edges: SSAB Boron width tolerances are corresponding to -0/+2 mm.

Shape

Hot rolled strip: according to EN 10051. Narrower tolerances are available on request.

Flatness

Hot rolled sheets: SSAB Boron tolerances guarantee a maximum flatness deviation of 6 mm/m in addition to the EN 10051 flatness requirements. Flatness guarantees only apply for cut to length sheets.

Surface Properties

Hot rolled strip products: According to EN 10163-2 Class A, Subclass 3.

Delivery Conditions

Hot rolled coils and sheets are delivered in as-rolled or by separate agreement annealed condition.

Surface Condition

Hot rolled strip products are available in non-pickled, pickled dry or pickled & oiled condition.

Fabrication and Other Recommendations

For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.

Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.

Contact Information

www.ssab.com/contact