GreenCoat TSP Pural BT color coated steel is available in matt, metallic and satin finishes and offers a wide range of colors inspired by Nordic nature. It provides a coating where rapeseed oil and other renewable raw materials are used. SSAB has long experience of Bio-based Technology (BT) in GreenCoat® products.
This product has been developed together with tinsmiths in order to obtain optimum product properties combined with Nordic quality steel and an excellent coating. The result is a unique, premium product for tinsmiths.
GreenCoat TSP Pural BT offers the highest level of durability for standing-seam systems and can be used in all premium tinsmith applications. The formable TSP (TinSmith Pro) steel has practically no spring back, which allows for very tight folding.
GreenCoat TSP Pural BT color coated steel offers a coating that is optimized to resist weathering, resulting in excellent UV resistance (Ruv5 for matt appearance) and corrosion classes (RC5+). The product has excellent scratch resistance and is easy to handle during manufacturing. GreenCoat TSP Pural BT is highly formable and workable at temperatures down to – 15°C, allowing for year-round installation at lower costs.
The newly developed satin appearance of GreenCoat TSP Pural BT responds well to current architectural and design trends. It has a gloss level of 20.
The reverse side of the sheet is painted with a two-layer grey backside coating.
GreenCoat TSP Pural BT complies with current REACH regulations and is fully chromate free.
SSAB’s color coated steels are all manufactured according to EN 10169.
GreenCoat and Pural are trademarks of the SSAB group of companies.
1) Classification into corrosion resistance categories is based on blistering, delamination and damage on bend of the coating after four years exposure in natural outdoor testing sites as specified in EN 10169.
2) TSP fulfills the requirements of EN 10346 DX53D.
Below are the colors currently available. Other colors can be agreed upon separately.
Colors shown in the color table are only indicative. To see the real visual appearance of the product, please order a color sample. Please note also that the same colors between the products may differ.
For information on thermal properties (solar reflectance index SRI or thermal emittance TE) of available colors, please contact SSAB Tech Support.
Note especially for Metallic and all Matt colors: To ensure tonal consistency of colors on a single exterior face, all material must come from the same production batch. Also the directionality of surfaces has to be consistent especially when sheets are cut to size. Compared to solid colors, larger measured color variation between production batches is typical for metallic colors, even if color is visually stable.
Unless otherwise specified, the reverse side of the sheet is painted with a two-layer coating to further improve the corrosion resistance of the end product. The coating provides good adhesion properties to many adhesives and foams; nevertheless the compatibility needs to be tested case-specifically.
For easy material identification the reverse side of the sheet is stamped with the GreenCoat logo and the product name. The production date is marked to ease material traceability and can be referred to within the guarantee period. An arrow shows the direction of production to ensure installation in a uniform direction.