Product Name | Dimensions | Mechanical properties | Datasheet |
---|---|---|---|
ERB 120/120+ |
Profile diameter: 27.00 mm Original tube diameter: 41.00 mm Upper bushing diameter: 27.99 mm Bushing head diameter: 30.00 - 37.01 mm Standard length *: 1500.0 - 3999.99 mmProfile diameter: 27 mm Original tube diameter: 41 mm Upper bushing diameter: 28 mm Bushing head diameter: 30 - 37 mm Standard length *: 1500 - 4000 mm |
Walll thickness: 2.0 mm Minimum yield load : 5.054 kN Typical elongation A: 15 - 30 % Elongation A (Min): 10 - 20 % Typical breaking load (not guaranteed): 6.571 kN Minimum breaking load: 6.063 kN |
|
ERB 160/160+ |
Profile diameter: 35.99 mm Original tube diameter: 54.00 mm Upper bushing diameter: 38.00 mm Bushing head diameter: 41.00 - 48.01 mm Standard length *: 2400.0 - 5999.99 mmProfile diameter: 36 mm Original tube diameter: 54 mm Upper bushing diameter: 38 mm Bushing head diameter: 41 - 48 mm Standard length *: 2400 - 6000 mm |
Walll thickness: 2.0 mm Minimum yield load : 6.063 - 6.571 kN Typical elongation A: 15 - 30 % Elongation A (Min): 10 - 20 % Typical breaking load (not guaranteed): 8.086 - 8.594 kN Minimum breaking load: 8.086 kN |
|
ERB 240/240+ |
Profile diameter: 35.99 mm Original tube diameter: 54.00 mm Upper bushing diameter: 38.00 mm Bushing head diameter: 41.00 - 48.01 mm Standard length *: 2400.0 - 5999.99 mmProfile diameter: 36 mm Original tube diameter: 54 mm Upper bushing diameter: 38 mm Bushing head diameter: 41 - 48 mm Standard length *: 2400 - 6000 mm |
Walll thickness: 3.00 mm Minimum yield load : 8.592 - 10.11 kN Typical elongation A: 15 - 30 % Elongation A (Min): 10 - 20 % Typical breaking load (not guaranteed): 12.13 - 12.6 kN Minimum breaking load: 11.6 - 12.13 kNWalll thickness: 3.0 mm Minimum yield load : 8.592 - 10.11 kN Typical elongation A: 15 - 30 % Elongation A (Min): 10 - 20 % Typical breaking load (not guaranteed): 12.13 - 12.6 kN Minimum breaking load: 11.6 - 12.13 kN |