Strenx® Tube 960QLH
Advanced high-strength structural hollow sections
Strenx® Tube 960QLH is plasma-welded, quenched and tempered hollow section with a minimum yield strength of 960 MPa.
Its high strength, combined with naturally stiff form of the welded hollow section, enables construction of stronger and lighter structures. Strenx® Tube 960QLH meets or exceeds the requirements of prEN 10210 (2016).
Typical applications are load-bearing lattice structures in the lifting, material handling and transportation sectors, especially in conditions where extremely good toughness is needed.