180
Strenx Tube 960QLH

Strenx® Tube 960QLH

Advanced high-strength structural hollow sections

Strenx® Tube 960QLH is plasma-welded, quenched and tempered hollow section with a minimum yield strength of 960 MPa.

Its high strength, combined with naturally stiff form of the welded hollow section, enables construction of stronger and lighter structures. Strenx® Tube 960QLH meets or exceeds the requirements of prEN 10210 (2016).

Typical applications are load-bearing lattice structures in the lifting, material handling and transportation sectors, especially in conditions where extremely good toughness is needed.

Dimension Range

Strenx® Tube 960QLH is available at circular shape.

   
Circular (mm)   76.1 - 133.0
Wall thickness (mm)       3.0 - 6.0 
Mill length (mm)   6000 - 12 000 

Available Standards

EN 10210-2

Strenx® Tube 960QLH

Strenx® Tube 960QLH

USED FOR
STANDARDS
DATA SHEET
USED FOR

Structural

Engineering

STANDARDS

EN 10210-2

DATA SHEET