Customer case

Streamlined savings

November 07, 2018 6 min read

""

Case details

Industry Trailers and body builders

The containers on this truck and trailer combination were upgraded from S235 standard steel to Strenx® 700MC, saving 560 kg per container. This increases the payload per trip by 1,680 kg for the total vehicle with three containers and also reduces the fuel consumption for the empty vehicle. Through an optimised design the wind drag is reduced, which further reduces the fuel consumption.

SSAB EcoUpgraded

Together with our customers, SSAB continually upgrades steel and equipment designs. SSAB EcoUpgraded saves CO2 both in steel production and during the full lifetime of the machine.

From the CO2 payback time and onwards, every extra hour brings additional savings.

EcoUpgraded logo

Savings on CO₂

SSAB EcoUpgraded Roll-on containers
  Calculation data
Fuel consumption, fully loaded 68 litres/100 km
Fuel consumption,without load 30 litres/100 km
Machine usage per year 100 000 km/year
Distance with maximum load 50%
Service lifetime 12 years 
Maximum payload (before upgrading) 34 200 kg
Gross weight (fully loaded) 64 000 kg
Weight of original parts 9 300 kg
Weight of upgraded parts
7 620 kg
180