SSAB Form 200 Cold-Rolled
A mild steel for modern production methods
SSAB Form 200 is a mild steel intended for forming with the best conceivable properties in both drawing and stretch forming operations. SSAB Form 200 is used for a wide variety of applications including vehicle parts, refrigerators, electric radiators and water radiators.
SSAB Form 200 offers consistent properties that assist modern, rapid production methods.