Hardox® 500

The bendable, weldable and highly abrasion-resistant steel.

Hardox® 500 is a bendable and weldable abrasion-resistant steel, with a nominal hardness of 500 HBW. Suitable for applications that demand higher wear resistance.

Hardox® 500 increases payload and increases service life while maintaining good processability and toughness.

 

Order trial material Get free technical advice

What is hardness?

Learn about our customers success when using Hardox wear plate

Dimension Range

Hardox® 500 is available as plate in thicknesses of 4.0 – 103.0 mm and as sheet in thicknesses of 2.0 - 7.0 mm. Hardox® 500 plate is available in widths up to 3350 mm and lengths up to 14630 mm. Hardox® 500 sheet is available in widths up to 1650 mm and lengths up to 16000 mm. More detailed information on dimensions is provided in the dimension program.

 

Available Standards

EN 10029

EN 10051

Hardox® 500

Hardox® 500

USED FOR
DIMENSIONS
STANDARDS
DATA SHEET
USED FOR

Wear Resistant

DIMENSIONS

T: 2 - 103 mm

W: Up to 3350 mm

L: Up to 14630 mm

STANDARDS

EN 10029

EN 10051

DATA SHEET