GreenCoat RWS Pural is an excellent product for rainwater system applications and features a highly durable, double-sided coating developed specifically for high quality rainwater systems.

GreenCoat RWS Pural provides excellent corrosion resistance, gloss retention and color fastness. It is also highly flexible, allowing for the ­forming of various products. Thanks to its slightly structured surface, GreenCoat RWS Pural sheds dirt and debris easily and remains clean in use. 

GreenCoat RWS Pural has excellent weather resistance. Depending on the environmental conditions, the product may retain its aesthetic ­properties for over 30 years. The regular maintenance and cleaning of rainwater systems will significantly prolong the service life of the product.

SSAB color coated steels comply with current REACH regulations and are fully free of chromates. Color coated steels are all manufactured according to EN 10169 + A1.

Product details

In this section, you will find the wide range of GreenCoat® color coated products for roofing applications including technical details.
Learn more

Product details

In this section, you will find our wide product offering with our Nordic quality steels and zinc coatings recommended for different applications. Details about product dimensions are also available.

Main applications  Recommended product*  Recommended steels Recommended Zinc mass Min thickness**  Width range*** 
Roofing, tinsmith
GreenCoat PLX Pro BT PLX Z350 0.60 mm 1000-1500 mm
 GreenCoat FAP Pro BT FAP  Z350  0.60 mm 1000-1500 mm 
GreenCoat PLX Legacy PLX Z350 0.60 mm 1000-1500 mm
           
Roofing, tiles & profiles GreenCoat Pural BT S280GD, S320GD, S350GD
Z275 0.50 mm 1000-1500 mm
GreenCoat Pro BT S280GD, S320GD, S350GD
Z275 0.50 mm 1000-1500 mm
GreenCoat Mica BT S280GD, S320GD, S350GD
Z275 0.50 mm 1000-1500 mm
GreenCoat Crown BT S280GD, S320GD, S350GD
Z275 0.50 mm 1000-1300 mm
Rough Matt Polyester S280GD, S320GD, S350GD
 Z275 0.45 mm  1000-1424 mm
Polyester S280GD-S350GD, DX51D
Z275 0.42 mm 1000-1500 mm
           
Roofing, modular GreenCoat Crown BT S280GD, S320GD, S350GD Z275 0.50 mm 1000-1300 mm
           
Rain water systems GreenCoat RWS Pro FAX, PLX Z275 0.50 mm 1000-1500 mm
           
Facades GreenCoat Hiarc S280GD, S320GD, DX51D 
Z275 0.50 mm 1000-1500 mm
GreenCoat Hiarc Max S280GD, S320GD, DX51D 
Z275 0.50 mm 1000-1500 mm
GreenCoat Anti-Graffiti BT S280GD, S320GD, DX51D 
Z275 0.50 mm 1000-1500 mm
GreenCoat Crown BT S280GD, S320GD
Z275 0.50 mm 1000-1300 mm
Polyester S280GD, S320GD, DX51D 
Z275 0.42 mm 1000-1500 mm
           
Indoor applications Polyester Indoor S250GD-S350GD, DX51D 
Z100 0.40 mm 1000-1424 mm
GreenCoat Foodsafe BT S250GD-S350GD, DX51D 
Z100 0.50 mm 1000-1500 mm
Laminate Foodsafe S250GD-S350GD, DX51D 
Z275 0.42 mm 1000-1400 mm
Epoxy S250GD-S350GD, DX51D 
Z100 0.40 mm 1000-1500 mm

* In addition to these we have a wide range of so called custom made products. Please contact SSAB Europe Tech support.
** Please take into account the country specific building recommendations concerning the minimum thickness. If other thicknesses are required, please contact SSAB Tech Support. Max thickness is 1,5 mm.
*** Max width depends on steel thickness. If other steel dimensions are needed, please contact SSAB Tech Support.

GreenCoat coils

GreenCoat RWS Pural

GreenCoat RWS Pural

USED FOR
MAIN PROPERTIES
COATING
COLOR PALETTE
DATA SHEET
USED FOR

Rainwater systems

MAIN PROPERTIES

COATING

COLOR PALETTE

  • Winter White
    RR20 / SS0005

  • Pebble Grey
    RR21 / SS0011

  • Stone Grey
    RR22 / SS0554

  • Mountain Grey
    RR23 / SS0036

  • Nordic Night Black
    RR33 / SS0015

  • Walnut Brown
    RR32 / SS0387

  • Chestnut Brown
    RR887 / SS0435

  • Cottage Red
    RR29 / SS0758

  • Pine Green
    RR11 / SS0830

DATA SHEET