Highly formable tinsmith product with special surface for applications to be painted directly after installation

GreenCoat PLX Legacy is a product for old cultural buildings’ roofs to be renovated

GreenCoat PLX Legacy is a product for tinsmith applications where the roof and coverings will be painted on site giving traditional handcrafted appearance. Typical applications are old cultural historic buildings’ roofs to be renovated.

GreenCoat PLX Legacy is highly suited and also recommended to be painted immediately after installation on worksite. It does not need weathering period or primer painting like pure zinc coated roofs. The coating has been optimised for good adhesion with air drying paints and high friction for safe working on the roof.

The product has the highly formable PLX steel. This means that the product is recommended for long-strip roofing providing very tight folding.

The reverse side is protected with grey reverse side coating which improves the corrosion resistance of the end product. SSAB color coated products comply with current REACH regulations and are fully free of chromates. GreenCoat® color coated steels are all manufactured according to EN 10169 + A1.

Product details

In this section, you will find the wide range of GreenCoat® color coated products for roofing applications including technical details.
Learn more

Product details

In this section, you will find our wide product offering with our Nordic quality steels and zinc coatings recommended for different applications. Details about product dimensions are also available.

Main applications  Recommended product*  Recommended steels Recommended Zinc mass Min thickness**  Width range*** 
Roofing, tinsmith
GreenCoat PLX Pro BT PLX Z350 0.60 mm 1000-1500 mm
 GreenCoat FAP Pro BT FAP  Z350  0.60 mm 1000-1500 mm 
GreenCoat PLX Legacy PLX Z350 0.60 mm 1000-1500 mm
           
Roofing, tiles & profiles GreenCoat Pural BT S280GD, S320GD, S350GD
Z275 0.50 mm 1000-1500 mm
GreenCoat Pro BT S280GD, S320GD, S350GD
Z275 0.50 mm 1000-1500 mm
GreenCoat Mica BT S280GD, S320GD, S350GD
Z275 0.50 mm 1000-1500 mm
GreenCoat Crown BT S280GD, S320GD, S350GD
Z275 0.50 mm 1000-1300 mm
Rough Matt Polyester S280GD, S320GD, S350GD
 Z275 0.45 mm  1000-1424 mm
Polyester S280GD-S350GD, DX51D
Z275 0.42 mm 1000-1500 mm
           
Roofing, modular GreenCoat Crown BT S280GD, S320GD, S350GD Z275 0.50 mm 1000-1300 mm
           
Rain water systems GreenCoat RWS FAX, PLX Z275 0.50 mm 1000-1500 mm
           
Facades GreenCoat Hiarc S280GD, S320GD, DX51D 
Z275 0.50 mm 1000-1500 mm
GreenCoat Hiarc Max S280GD, S320GD, DX51D 
Z275 0.50 mm 1000-1500 mm
GreenCoat Anti-Graffiti BT S280GD, S320GD, DX51D 
Z275 0.50 mm 1000-1500 mm
GreenCoat Crown BT S280GD, S320GD
Z275 0.50 mm 1000-1300 mm
Polyester S280GD, S320GD, DX51D 
Z275 0.42 mm 1000-1500 mm
           
Indoor applications Polyester Indoor S250GD-S350GD, DX51D 
Z100 0.40 mm 1000-1424 mm
GreenCoat Foodsafe BT S250GD-S350GD, DX51D 
Z100 0.50 mm 1000-1500 mm
Laminate Foodsafe S250GD-S350GD, DX51D 
Z275 0.42 mm 1000-1400 mm
Epoxy S250GD-S350GD, DX51D 
Z100 0.40 mm 1000-1500 mm

* In addition to these we have a wide range of so called custom made products. Please contact SSAB Europe Tech support.
** Please take into account the country specific building recommendations concerning the minimum thickness. If other thicknesses are required, please contact SSAB Tech Support. Max thickness is 1,5 mm.
*** Max width depends on steel thickness. If other steel dimensions are needed, please contact SSAB Tech Support.

GreenCoat coils

GreenCoat PLX Legacy

GreenCoat PLX Legacy

USED FOR
MAIN PROPERTIES
COATING
COLOR PALETTE
DATA SHEET
USED FOR

Roofing

MAIN PROPERTIES

Enhanced formability

COATING

COLOR PALETTE

  • Grey
    RR2P1 / SS0916

DATA SHEET