GreenCoat Hiarc
It offers a PVDF-based coating specially developed for facades and cassettes
It offers a PVDF-based coating specially developed for facades and cassettes
GreenCoat Hiarc is available in Regular and Matt finishes and now also with Shine Effect. Regular and Matt finishes has a wide range of attractive colors as well as metallic colors with long production experience resulting good color and gloss consistency. Shine Effect has through multilayer coating a special appearance providing glittery but coloured appearance and excellent properties.
GreenCoat Hiarc is a product targeted to high-end facades where the demands are high, but can be used also in roofing applications. GreenCoat Hiarc possesses excellent weather resistance properties and tolerates forming well. However, if extended corrosion properties are required, such as for buildings near a coastline, we offer GreenCoat Hiarc Max, which provides the necessary properties for this environment. Since the coating contains fluorine, the surface stays cleaner compared to other products. The coating is also easy to clean due to hard surface. If needed, strippable protective films are available for this product.
The reverse side of the sheet is painted as standard with a two-layer grey backside coating. SSAB color coated products comply with current REACH regulations and are fully free of chromates. GreenCoat® color coated steels are all manufactured according to EN 10169 + A1.