GreenCoat Cool acts as a heat shield for your building.
GreenCoat Cool for roofing features special solar heat reflecting properties that make the surface stay cooler than regular coated surfaces. For buildings that need cooling, this product helps to save energy and increases the thermal comfort.
The largest difference in surface temperature between GreenCoat Cool and standard products is achieved for dark colors.
In the table below you will find typical values for some colors. Total solar reflectance¹ and Thermal IR emittance² describes the product properties.
The reverse side of the sheet is painted as standard with a two-layer grey backside coating.
SSAB color coated products comply with current REACH regulations and are fully free of chromates. GreenCoat® color coated steels are all manufactured according to EN 10169 + A1.